ASTM A815 UNS 32760 Buttweld Fittings
video

ASTM A815 UNS 32760 Buttweld Fittings

UNS S32760 is a grade of super duplex stainless steel, which means it has a higher corrosion resistance and mechanical strength compared to standard duplex stainless steels. It contains a balanced combination of austenitic and ferritic microstructures, offering improved resistance to localized corrosion, pitting, crevice corrosion, and stress corrosion cracking.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of astm a815 uns 32760 buttweld fittings in China. If you're going to wholesale high quality astm a815 uns 32760 buttweld fittings made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

ASTM A815 UNS 32760 Buttweld Fittings

Product Introduction

ASTM A815 UNS S32760 is a specification established by the American Society for Testing and Materials (ASTM) that covers the standard requirements for wrought ferritic, austenitic, and duplex steel butt-welding fittings. These fittings are intended for use in various high-corrosion and high-strength environments, making them suitable for applications in industries such as oil and gas, petrochemical, chemical processing, and more.

Butt-weld fitting are components used to connect pipes and tubes, allowing for a seamless and leak-proof connection. They are widely used in piping systems where fluid flow and containment are critical. ASTM A815 UNS S32760 buttweld fitting are manufactured through a welding process that involves joining two pieces of pipe or tubing by heating them and then fusing them together.

Specifications of Super Duplex Steel UNS S32760 Butt weld Fitting

STANDARD UNS WERKSTOFF NR.
Super Duplex S2760 S32760 1.4410

Super Duplex Steel UNS S32760 Butt weld Fitting Chemical Composition

UNS S32760

C
N
P
Si
Mn
Mo
Ni
Cr
S
Other
0.030
0.24/0.32
0.035
0.80
1.20
3.0/5.0
6.00/8.00
24.0/26.0
0.020
Cu:0.50

Mechanical Properties of Super Duplex Steel UNS S32760 Butt weld Fitting

UNS Grade

Proof Stress

0.2% (MPa)

Tensile Strength

(MPa)

Elongation

A5(%)

Hardness Max
HB HRB
S32760 2507 550 795 15 310 32*

buttweld fitting