Copper Nickel 70/30 Seamless Pipe
video

Copper Nickel 70/30 Seamless Pipe

Copper Nickel 70/30 Seamless Tube has good strength and flexibility, making it easy to fabricate and install. Its high thermal conductivity and resistance to biofouling make it ideal for heat exchangers and condensers.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of copper nickel 70/30 seamless pipe in China. If you're going to wholesale high quality copper nickel 70/30 seamless pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Copper Nickel 70/30 Seamless Pipe

Product Introduction

Copper Nickel 70/30 Seamless Pipe is a pipe material made from a specific copper-nickel alloy composition. The term "70/30" refers to the copper-nickel ratio in the alloy, meaning it contains approximately 70% copper and 30% nickel. This special composition gives the seamless pipe unique properties. Copper Nickel 70/30 Seamless Pipe has excellent corrosion resistance, making it suitable for applications in marine environments or those involving saltwater exposure.

Chemical Composition Of ASTM B466 C71500 Copper Nickel Seamless Pipes And Tubes

The chemical composition of UNS C71500 copper nickel alloys is outlined in the following table.

Element Content (%)
Copper, Cu 70.0
Nickel, Ni 30.0

Physical Properties ASTM B466 C71500 Copper Nickel Seamless Pipes And Tubes

The following table shows the physical properties of UNS C71500 copper nickel alloys.

Properties Metric Imperial
Density 8.94 g/cm3 0.323 lb/in3
Melting point 2140°F 1171°C

Mechanical Properties ASTM B466 C71500 Copper Nickel Seamless Pipes And Tubes

The Mechanical Properties of UNS C71500 copper nickel alloys are displayed in the following table.

Properties Metric Imperial
Tensile strength, ultimate 372-517 MPa 54000-75000 psi
Tensile strength, yield (depending on temper) 88.0-483 MPa 12800-70100 psi
Elongation at break (in 381 mm) 45.0% 45.0%
Charpy impact 107 J 78.9 ft-lb
Machinability (UNS C36000 (free-cutting brass) = 100%) 20% 20%
Shear modulus 57.0 GPa 8270 ksi
Poisson's ratio 0.34 0.34
Elastic modulus 150 GPa 21800 ksi

copper nickel piping

Hot Tags: copper nickel 70/30 seamless pipe, China copper nickel 70/30 seamless pipe suppliers, C12000 Copper Alloy Pipe

Send Inquiry

whatsapp

Phone

E-mail

Inquiry