Aluminum Alloy 7075 Bar
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of aluminum alloy 7075 bar in China. If you're going to wholesale high quality aluminum alloy 7075 bar made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Products Description
Aluminum Alloy 7075 Bar
7075 is one of the highest strength aluminum alloys. It has good fatigue strength and average machinability. Often used where parts are highly stressed. It is not weld able and has less corrosion resistance than other aluminum alloys. The mechanical properties depend on the temper of the material. Commonly used in the bicycle industry, aircraft structures, and in rifles for the American military.
Products Properties
Alloy 7075 Chemical Composotion:
|
Chemical Composition Limits |
|||||||||||
|
Weight% |
Al |
Si |
Fe |
Cu |
Mn |
Mg |
Cr |
Zn |
Ti |
Other Each |
Others Total |
|
7075 min |
Rem |
- |
- |
1.2 |
- |
2.1 |
0.18 |
5.1 |
- |
- |
- |
|
7075 max |
Rem |
0.40 |
0.50 |
2.0 |
0.30 |
2.9 |
0.28 |
6.1 |
0.20 |
0.05 |
0.15 |
Typical Mechanical Properties:
|
Material |
Temper |
Size (") |
Tensile Strength (ksi) |
Yield Strength (ksi) |
Elongation in 2" % |
|
Alloy 7075 Bar |
T651 |
- |
77 |
66 |
7 |
|
Alloy 7075 Bar |
T7351 |
<4" |
68 |
56 |
10 |
|
Alloy 7075 Bar |
T73511 |
<0.25 |
68 |
58 |
7 |
|
Alloy 7075 Bar |
T73511 |
0.25 - 1.5 |
70 |
61 |
8 |
|
Alloy 7075 Bar |
T73511 |
1.5 - 3.0 |
69 |
59 |
8 |
|
Alloy 7075 Bar |
T6511 |
<0.25 |
78 |
70 |
7 |
|
Alloy 7075 Bar |
T6511 |
0.25 - 0.5 |
81 |
73 |
7 |
|
Alloy 7075 Bar |
T6511 |
0.5 - 3.0 |
81 |
72 |
7 |
Aluminum Alloy 7075 Bar
Aluminum 7075 is a high-strength alloy that offers good stress-corrosion cracking resistance. Known as a mainstay in the aerospace industry since it was introduced, Aluminum 7075 brings moderate toughness as well as an excellent strength-to-weight ratio. It is also important to note that at sub-zero temperatures Aluminum 7075 increases in strength.
When it comes to welding, the resistance welding is preferred, while gas and arc welding should be avoided. It is available in in the clad (Alclad) form to improve corrosion resistance.
Customer Case

FAQ
Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.
Q:What shipping ports are there?
A:We normally ship from Shanghai,Tianjin, Qingdao, and Ningbo ports.
Q:What are your payment terms?
A:30% T/T in advance and 70% balance before shipment or based on BL copy or LC at sight.
Q:What about product pricing information?
A:Prices vary due to changes in raw material prices on a regular basis.
Q:Is it possible to send samples?
A:Of course, we offer free samples and express shipping to customers all over the world.
Q:Do you offer a service for customized products?
A:Yes, we can produce according to your specifications and drawings.