Aluminium Alloy 6061 Sheets And Plates
video

Aluminium Alloy 6061 Sheets And Plates

We utilize premium quality raw material for fabricating alloy 6061 sheets and plates as per the universal quality guidelines. Cutting edge tools and machines are utilized for making a high and valuable range of Aluminium alloy 6061 sheets and plates. At the same time, fabricating these items, national and global specifications are included in the material to create high-quality items. Several features are included in aluminium alloys 6061 sheets and plates such as machineability, high strength, formability, and corrosion resistance.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of aluminium alloy 6061 sheets and plates in China. If you're going to wholesale high quality aluminium alloy 6061 sheets and plates made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

We utilize premium quality raw material for fabricating alloy 6061 sheets and plates as per the universal quality guidelines. Cutting edge tools and machines are utilized for making a high and valuable range of Aluminium alloy 6061 sheets and plates. At the same time, fabricating these items, national and global specifications are included in the material to create high-quality items. Several features are included in aluminium alloys 6061 sheets and plates such as machineability, high strength, formability, and corrosion resistance.

4 99

Alloy 6061 aluminium plates are full-proof quality and high utility power. This tooling plate exhibits exceptional machinability, weldability, and average strength intensively than most alloys. Aluminium Alloy 6061 is customarily selected where welding or brazing is necessary or for its high corrosion resistance in all range.

UNS EN DIN ISO BS (OLD) USA WNR
A96061 EN AW-6061 AlMgSiCu AlMg1SiCu HE20 AA6061 3.3211

4 200

 

Mn Si Cr Cu Fe Zn Al Mg Ti Other Each/Total
0.15 0.4-0.8 0.15-0.35 0.15-0.4 0.7 0.25 Remainder 0.8-1.2 0.15 0.005/0.15

In addition, it has extraordinary joining features, good acceptance anodizing, and is simply cold worked and created in the annealed condition. Aluminium Alloy 6061 is mainly a precipitation-hardened aluminium alloy that possesses silicon and magnesium as the critical alloying elements. This alloy is also known as alloy 61S and has good quality physical and mechanical properties. Aluminium Alloy 6061 Sheet and Plate are used for both general and for industrial purposes. We maintain highest qualities of our products.
 

Hot Tags: aluminium alloy 6061 sheets and plates, China aluminium alloy 6061 sheets and plates suppliers, 5052 Aluminium Sheet Plate, Checker Aluminium Sheet Plate, 6082 T6 Aluminium Sheet Plate