Super Alloy 2.4669 Nickel Base Plate
video

Super Alloy 2.4669 Nickel Base Plate

Nickel (plus cobalt)…70.00 minutes Chromium…14.0-17.0 Iron…5.0-9.0 Titanium…2.25-2.75 Aluminum…0.40-1.00 Niobium (plus tantalum)…0.70-1.20 Manganese…1.00 Max. Silicon…below 0.50 Sulfur…below 0.01 Copper…0.50 or less Carbon…0.08 or less Cobalt 1 …1.00 Max
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of super alloy 2.4669 nickel base plate in China. If you're going to wholesale high quality super alloy 2.4669 nickel base plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Super alloy 2.4669 Nickel Base Plate

2.4669 Nickel Base Superalloy Plate is a corrosion-resistant, oxidation-resistant, high-strength precipitation hardening alloy. It is mainly a nickel-based high-temperature alloy that is age-strengthened with the γ" phase. The service temperature is below 800°C. The alloy has good corrosion resistance and oxidation resistance below 980°C, and has high strength below 800°C. It has good creep resistance below 700℃ and good relaxation resistance below 540℃. It also has good formability and welding performance. The alloy is in solid solution state and is pure austenite. body tissue.

 

2.4669 Nickel Base Superalloy Plate

 

Grade

Ni%

Cr%

Nb%

Fe%

Al%

Ti%

C%

Mn%

Si%

Cu%

S%

Co%

Inconel X750

Max 70

14-17

0.7-1.2

5.0-9.0

0.4-1.0

2.25-2.75

Max 0.08

Max 1.00

Max 0.50

Max 0.5

Max 0.01

Max 1.0

 

2.4669 Nickel Base Superalloy Plate Application

 

Rocket construction

Components for gas turbines

Nuclear reactors

Tools

Aircraft structure

Hot Tags: super alloy 2.4669 nickel base plate, China super alloy 2.4669 nickel base plate suppliers, oxidation resistant alloy, strong alloy, durable alloy, precision alloy, advanced alloy, engineering alloy

Send Inquiry

whatsapp

Phone

E-mail

Inquiry