Name: Nickel 201 Bright Annealed Pipe
Approximate grades:NO2201,Nickel201,Ni201,N5
Shape:Round
Technique:Cold Rolled
Tolerance:-+10%
Processing Service:Bending, Welding, Decoiling, Punching, Cutting
Pipe Form Type:Seamless Steel Pipe
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of nickel 201 bright annealed pipe in China. If you're going to wholesale high quality nickel 201 bright annealed pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Nickel 201 Annealed Tube Compared to Nickel 200, Nickel 201 is a low carbon variety with low annealing hardness and very low work hardening rate, which is ideal for cold forming operations. It is highly resistant to corrosion from neutral and alkaline salt solutions, fluorine and chlorine, but will corrode severely in oxidizing salt solutions.

 

Pure Nickel 201 Seamless Tube Applications
Includes food and synthetic fiber processing equipment, electronic parts, aerospace and missile components, and treatment with sodium hydroxide above 300°C.

 Nickel 201 Specification

 Nickel 201 high precision Tube Chemical Composition

Grade

Ni

Cu

Fe

Mn

C

Si

S

UNS N02201

≥99.01

≤0.25

≤0.40

≤0.35

≤0.02

≤0.35

≤0.01

 

Nickel Alloy 201 Thin Wall Pipe Mechanical Properties

Grade

Condition

Tensile Strength

Yield Strength

Elongation(%)

N02201

Annealed

≥50(345)ksi(MPa)

≥12(83)ksi(MPa)

≥40

N02201

OD≤127MM

Annealed

≥50000(380)psi(MPa)

≥12000(80)psi(MPa)

≥35

N02201

OD>127MM

Annealed

≥50000(345)psi(MPa)

≥10000(70)psi(MPa)

≥40

 Alloys 201 Products Display

UNS N02201 Nickel clad pipe

UNS N02201 Nickel clad pipe

Why choosing GNEE

GNEE has 10+ spot warehouses. The annual supply capacity is about 10 million tons. It has 16 years of experience in supplying large projects. The customer return rate is 86%. The company promises that all products are of guaranteed quality and quantity, and can provide material certification and three-party inspection. If you are not satisfied, you can get a refund. You can buy with confidence.

please contact us for a quote! ss@gneesteel.com

PRODUCTS TESTING

Nickel 201 Alloy Pipe for Condenser Tube

nickel 201 suppliers

Nickel  201 Alloy Manufacturer

 Alloy 201 Seamless Pipe Manufacturer

 Superalloys 201 Pipe Supplier, Stockist

FAQ

Q:What about product pricing information?
Prices vary due to changes in raw material prices on a regular basis.

Q:Is it possible to send samples?
Of course, we offer free samples and express shipping to customers all over the world.

Q:Do you offer a service for customized products?
Yes, we can produce according to your specifications and drawings.

Hot Tags: nickel 201 bright annealed pipe, China nickel 201 bright annealed pipe suppliers, Monel 400 Alloy Steel Sheet, Alloy Steel 600 plate, Hastelloy C276 ROUND BAR, Hastelloy C 22 Alloy Steel Flange, Cold Rolled Inconel 625 Alloy Seamless Pipe, Nickel Alloy Coil B2

Send Inquiry

whatsapp

Phone

E-mail

Inquiry