Incoloy Alloy 800 Pipe
video

Incoloy Alloy 800 Pipe

Incoloy 800 is an Iron nickel chromium alloy with a low carbon content with good strength and resistance to oxidation and carburization to intermediate temperatures.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of incoloy alloy 800 pipe in China. If you're going to wholesale high quality incoloy alloy 800 pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Incoloy Alloy 800 pipe is an austenitic stainless steel alloy composed of iron, nickel and chromium. It is widely regarded as having excellent high temperature oxidation resistance and corrosion resistance. It is suitable for a variety of extreme environments, such as high temperature and highly corrosive media.
Material composition and basic properties
Chemical composition: Incoloy Alloy 800 is mainly composed of chromium, nickel and iron, of which the nickel content is very high, accounting for about 30%-35%.
Physical properties: The alloy has good thermal conductivity and low thermal expansion coefficient, which makes it stable in temperature-changing environments and not easy to deform.
Mechanical properties and processing characteristics
Strength and ductility: Incoloy Alloy 800 has high tensile strength and good ductility.
Welding performance: Incoloy Alloy 800 has excellent welding performance.
Corrosion resistance and high temperature resistance
Corrosion resistance: Due to its unique chemical composition, Incoloy Alloy 800 shows excellent corrosion resistance to a variety of acids and alkalis, including hydrochloric acid, sulfuric acid, etc. This corrosion resistance makes it an ideal material for handling corrosive media in the chemical and petrochemical industries.
High temperature oxidation resistance: Incoloy Alloy 800 can maintain stable performance at temperatures up to 1150°C, which makes it very suitable for high temperature applications such as heat treatment equipment and furnace structures.
Application areas and cases
Petrochemical industry: In the petrochemical industry, Incoloy Alloy 800 is used to manufacture key components such as heat exchange equipment, boiler feed water heaters, pipelines, containers, towers, tanks, valves, pumps, reactors, etc.

 

Incoloy UNS No 8800 Seamless Pipe Chemical Composition

Grade C Mn Si Fe S Cr Al-Ti Ni
Incoloy 800 Pipe min. – – – 39.5 – 19.0 0.15 30.0
max. 0.1 1.5 1.0 – 0.015 23.0 0.60 35.0
Incoloy 800H Pipe min. 0.05 – – 39.5 – 19.0 0.15 30.0
max. 0.1 1.5 1.0 – 0.015 23.0 0.60 35.0
Incoloy 800HT Pipe min. 0.06 – – 39.5 – 19.0 0.85/0.25 30.0
max. 0.1 1.5 1.0 – 0.015 23.0 1.20/0.60 35.0

 

ASME SB 167 UNS N08800 Incoloy Pipe Mechanical Properties

Grade Tensile Strength (MPa) min Yield Strength 0.2% Proof (MPa) min Elongation (% in 50mm) min Hardness
Rockwell B (HR B) max Brinell (HB) max
800-H-HT Psi – 75,000 , MPa – 520 Psi – 30,000 , MPa –205 30 – –

Incoloy 800 UNS N08800 Equivalent Material

STANDARD WERKSTOFF NR. UNS JIS BS GOST AFNOR EN OR
Incoloy 800 Pipe 1.4876 N08800 NCF 800 NA 15 ЭИ670 Z8NC32-21 X10NiCrAlTi32-20 XH32T
Incoloy 800H Pipe 1.4958 / 1.4876 N08810 NCF 800H NA 15(H) ЭИ670 Z8NC33-21 X5NiCrAlTi31-20 XH32T
Incoloy 800HT Pipe 1.4859 / 1.4876 N08811 NCF 800HT NA 15(HT) ЭИ670 – X8NiCrAlTi32-21 XH32T

Incoloy Alloy 800 pipeIncoloy Alloy 800 pipeIncoloy Alloy 800 pipe

 