Incoloy 926 890 Alloy Pipe
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of incoloy 926 890 alloy pipe in China. If you're going to wholesale high quality incoloy 926 890 alloy pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Incoloy 926 890 Alloy Pipe
Alloy 926 (N08926) alloy is a versatile material that can be used in many industrial fields: 1. Fire protection systems, seawater purification systems, hydraulic and perfusion piping systems in marine engineering. 2. Bleaching tank in cellulose pulp production. 3. Polished rods in corrosive oil wells. 4. Hose systems in marine engineering. 5. Pipelines, joints, gas flow systems, etc. in acid gas production. 6. Components in the flue gas desulfurization system.
Incoloy 926 high temperature alloy composition:
1. Inconel 625 nickel-based high-temperature alloy. The carbon content is 0.95%, the chromium content is 11.5%, the molybdenum content is about 1.5%, the aluminum content is 0.15%, and the copper content is 0.5%.
2. Cadenati-Hafnung cobalt-based heat-resistant alloy, containing about 12.5% chromium and 6.2% nickel.
3. Timetrel ferritic stainless steel, iron content is 8-10%, carbon and sulfur are 0.08-0.2%.
The above three ingredients are the main ingredients of INCOLY 926. Other elements include Ni, Co, Cu, Cr, etc. Among them, Inconel 625 contains a small amount of Mo and Si; Timetrel contains a small amount of Mn; CADenato HAFNUNG contains a small amount of Fe and Ti.
Incoloy 926 main features:
1. It has good oxidation resistance and hydrogen embrittlement resistance below 1100°C. It has high thermal strength in the temperature range of 1150~1210°C (the thermal strength coefficient can reach 4W/mK), and also has good corrosion resistance and welding performance.
2. It has excellent cold deformation properties and high fracture toughness (strength factor greater than 400MPa/Mpa).
3. Due to the addition of a certain amount of Mo element, the thermal conductivity of the material is improved and the density is reduced, thereby increasing the strength limit and plasticity limit of steel.
4. It has excellent processing and forming process performance: it can smoothly carry out deep drawing and forming through various forms of cold stamping processing methods; it can easily carry out various forms of bending and forming processes and welding forming processes, etc.
Hot Tags: incoloy 926 890 alloy pipe, China incoloy 926 890 alloy pipe suppliers, wear resistant alloy, manufacturing alloy, construction alloy, Monel N04400 N05500 Thick Wall Pipe, advanced alloy, reliable alloy