Grade: GH3044
Surface treatment: 2B, 2D, BA NO(8)
Shape: round, square, rectangular
Type: seamless / ERW / welded
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of gh3044 gh747 heat resistant metals pipe in China. If you're going to wholesale high quality gh3044 gh747 heat resistant metals pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
GH3044 GH747 Heat Resistant Metals Pipe Products Description
GH3044 GH747 high temp alloys video
GNEE STEEL GROUP supplies GH3044 GH747 Heat Resistant Metals Pipe for you
Calculation formula for GH3044 steel
GH3044 flat bar: weight per meter (kg)=0.00785 × thickness × Edge width
GH3044 pipe: weight per meter (kg)=0.02466 × wall thickness × (Outer diameter wall thickness)
GH3044 bar: diameter * diameter * length * 0.00623 = kg/meter (weight per meter)
GH3044 plate: length * width * height * 0.00785=kg/meter (weight per meter)
| GNEE STEEL GH2747 Haynes 747 stainless Seamless Steel Pipe for industry | |
| Grade | Inconel Alloy GH2747 Haynes 747 |
| Diameter Of Alloy pipe | Hot Rolled: Φ8-38mm |
| Forging: Φ38-350mm | |
| Cold Rolled: ≤50mm | |
| Standard | ASTM AMSE YB HB BJB GB etc |
| Length | As Required |
| Surface | Black or Bright |
| Manufacture Technology | Hot Rolled ,Forging , Cold Rolled |
| Package | wooden boxes package,pvc package, and other package |
GH3044 GH747 Heat Resistant Metals Pipe chemical composition & Equivalent grade
GH3044 Heat Resistant Metals Pipe chemical composition
| Grade | GH3044 |
| Ni | Remainder |
| Cr | 23.5-26.5 |
| W | 13-16 |
| C | ≤0.1 |
| S | ≤0.013 |
| P | ≤0.013 |
| Fe | ≤4 |
| Ti | 0.3-0.7 |
| Cu | ≤0.25 |
| Al | ≤0.5 |
| Mo | ≤1.5 |
| Si | ≤0.8 |
| Mn | ≤0.5 |
GH747 Heat Resistant Metals Pipe chemical composition
| Element | C | Cr | Ni | Al | Fe |
| (%) | ≤0.10 | 15.00~17.00 | 44.00~46.00 | 2.90~3.90 | Blance |
| Eelment | Ce | Mn | Si | S | P |
| (%) | ≤0.030 | ≤1.00 | ≤1.00 | ≤0.020 | ≤0.025 |
GH3044 GH747 heat resistant metals Pipe


GH3044 is a Ni-Cr-based solid solution strengthened deformed high-temperature alloy with a service temperature below 900 degrees Celsius. The alloy contains large amounts of tungsten and small amounts of aluminum and titanium. The alloy has high plasticity and moderate thermal strength, and has excellent oxidation resistance and good new functions in stamping and welding processes.
GH2747 is a Fe-Ni-Cr-based precipitation hardening deformed high-temperature alloy. It is used in a solid solution state. Its long-term operating temperature is 1100℃-1250℃, and its short-term operating temperature can reach 1300℃. The high-temperature heat-resistant and anti-oxidation alloy GH2747 has high strength, good structural stability, and excellent anti-oxidation and corrosion resistance. The alloy has good weldability and can be welded using various processes.
GNEE Group Product Packaging
GH3044 GH747 Heat Resistant Pipe

GNEE Group Factory Environment
GH3044 GH747 Heat Resistant Pipe

Customer Case
customer visit

FAQ
Q: Can you provide us samples, is it free or does it require payment?
A: If you don't need to print your logo or other artwork on the product, we won't charge any fee, just tell us your freight collect account, such as Fedex, DHL, TNT. If you don't have it, we need to charge the express fee appropriately.
Q: Can I get your best price?
A: Our goal is to provide you with the best price and excellent quality assurance in the long run. Please leave your contact information to get the best quote, we will provide you with the best solution as soon as possible.
Q: About the product price of GH3044 GH747 heat resistant metals Pipe?
A: Due to cyclical changes in raw material prices, prices vary in different periods.
Contact Us
Address
No.4-1114 Beichen Building, Beicang Town, Beicheng District, Tianjin City, China
Phone
+86-15824687445
ss@gneesteel.com
Skype
mmkelly1314
Whatsapp/Wechat
+86 15824687445
Hot Tags: gh3044 gh747 heat resistant metals pipe, China gh3044 gh747 heat resistant metals pipe suppliers, Casting High Temperature Alloy
You Might Also Like
Send Inquiry