Stainless Steel SS304H Round Bar
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of stainless steel ss304h round bar in China. If you're going to wholesale high quality stainless steel ss304h round bar made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
SS 304H Round Bars is made with great physical and mechanical properties, which assists the bars to combine and get good quality and hardness to utilize within the relevant applications. These properties are elongation, support pressure loads, electrical conductivity, thickness, melting point, modulus of development, electrical conductivity, tensile strength, yield strength, extreme flexible quality, and electrical resistivity.
Furthermore, these bars are made with the assistance of the few chemicals that are best for the bars to induce resistivity properties. These chemicals are carbon, manganese, silicon, phosphorous, and many more. These bars are indeed outlined with detail like conditions, resilience, sorts, applications, surface, wrap up, conclusion, shapes, shape, measure, divider thickness, weight, length, width, and grade as well.
| Grade | UNS | DIN | JIS |
|---|---|---|---|
| SS 304H | S30409 | 1.4948 | SUS 304H |

| Chemical Composition of Stainless Steel 304H Round Bar | |||||||||
|---|---|---|---|---|---|---|---|---|---|
| Grade | C | Mn | Si | P | S | Cr | Mo | Ni | Cu |
| SS 304H | 0.10 max | 2 max | 0.75 max | 0.045 max | 0.03 max | 18 – 20 | – | 8 – 10.5 | - |

SS 304H Round Bars are utilized in numerous businesses like the sugar industry, oil industry, gas preparing, petrochemical industry, control era industry, control plant, claim to fame chemical industry, fertilizer industry, and dairy nourishment handling and breweries industry. Moreover, these bars are used for many applications such as heat exchangers, condensers, military applications, pumps, shafts, domestic apparatuses, as well.
SS 304H round Bars are best to use within the nourishment handling and capacity units since it is safe to the chemicals and chloride arrangements. These bars are made with universal properties and standards for sustention in ruthless situations. These bars are effortlessly maintained with the annealed temperatures without any distortion to the bars. Moreover, these bars are safe from the complete common corrosions.
Hot Tags: stainless steel ss304h round bar, China stainless steel ss304h round bar suppliers, Stainless Steel 446 Round Bar, 420 Stainless H type Steel, 304 316 Steel Flat Bars With Holes, Stainless Steel 310S Round Bar, 304 304L 316 316L Stainless Round Bar