Stainless Steel 15-5PH Round Bar & Rods
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of stainless steel 15-5ph round bar & rods in China. If you're going to wholesale high quality stainless steel 15-5ph round bar & rods made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
And the low-temperature hardening of the material improves the strength and allows the good fabrication along with the alloy. Also, with the excellent corrosion resistance feature, the alloy is suitable for all the applications. This is the way that the alloy is used in the development of the bars and rods.
Due to the presence of copper and nickel content the alloy made bars and rods are good at obtaining the corrosion resistance feature. The bars and rods are having pitting corrosion resistance and the best crevice corrosion resistance ability. Along with it, the bars and rods are having many other features. Some of the properties which the rods and bars are holding are great ductility, durability, high tensile strength, great toughness, stability in the elevated temperatures, weldability, and others. This is the reason that the types of bars and rods are used in the industries.
15-5PH STAINLESS STEEL ROUND BAR EQUIVALENT GRADES
| STANDARD | UNS | WNR. |
|---|---|---|
| SS 15-5PH | S15500 | 1.4545 |
CHEMICAL COMPOSITION OF STAINLESS STEEL 15-5PH ROUND BAR
| Grade | C | Cb+Ta | Cr | Cu | Fe | Mn | Ni | P | S | Si |
|---|---|---|---|---|---|---|---|---|---|---|
| SS 15-5 PH | 0.07 max | 0.15-0.45 max | 14.0-15.0 max | 2.5-4.5 max | Bal | 1.0 | 3.5-5.5 | 0.04 | 0.03 | 1.0 |
MECHANICAL PROPERTIES OF STAINLESS STEEL 15-5PH ROUND BAR
| Grade | Tensile Strength ksi (MPa) | Yield Strength 0.2% ksi (min) | Elongation % | Hardness (Rockwell) MAX |
|---|---|---|---|---|
| SS 15-5 PH | 161,000 | 140,000 | 7.6% | C35 |




Hot Tags: stainless steel 15-5ph round bar & rods, China stainless steel 15-5ph round bar & rods suppliers, 304 304L 316 316L Stainless Round Bar, Stainless Steel 310S Round Bar, Stainless Steel 446 Round Bar, 420 Stainless H type Steel, 304 316 Steel Flat Bars With Holes
You Might Also Like
Send Inquiry