S17700 17-7 PH AISI 631 Stainless Steel Bar 6 Mm Ch 900 Condition Heat Treatment
video

S17700 17-7 PH AISI 631 Stainless Steel Bar 6 Mm Ch 900 Condition Heat Treatment

S17700 17-7 PH AISI 631 Stainless Steel diameter 6 mm Ch 900 Condition Heat Treatment Aisi 631 / 17-7PH is an austenitic-martensitic precipitation hardening stainless steel developed on the basis of 18-8CrNi, also known as controlled phase transformation stainless steel. After solution treatment, it is an unstable austenite structure, which has good ductility and processability. After adjustment, the austenite precipitation and carbonization phenology components change, and then through martensitic transformation treatment, most of the structure is transformed into toughness. Better low-carbon tempered martensite, this state is the use state of steel, and has good mechanical properties at medium temperature. Corrosion resistance is better than general martensitic stainless steel.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of s17700 17-7 ph aisi 631 stainless steel bar 6 mm ch 900 condition heat treatment in China. If you're going to wholesale high quality s17700 17-7 ph aisi 631 stainless steel bar 6 mm ch 900 condition heat treatment made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

S17700 17-7 PH AISI 631 Stainless Steel Bar 6 Mm Ch 900 Condition Heat Treatment

Description

Certification: ISO,BV,SGS Type: Round
Application: Construction,decoration,Industry,Mechineal Standard: DIN,ASTM,AISI,JIS,EN
Grade: S17700 17-7 PH AISI 631 Shape: Round
Dimensions: 3mm-800mm Surface: Bright,Polished,black
Technique: Cold Drawn&hot Rolled Length: Customers' Requirements
Packing: Standard Seaworthy Package Price Term: CIF CFR FOB Ex-Work
Name: Heat Treatment H900 630/17-4Ph Stainless Steel Round Bar
High Light:

AISI 631 Stainless Steel Bar

,

Stainless Steel S17700 Bar

,

Stainless Steel Bar 6Mm

S17700 17-7 PH AISI 631 Stainless Steel diameter 6 mm Ch 900 Condition Heat Treatment

Aisi 631 / 17-7PH is an austenitic-martensitic precipitation hardening stainless steel developed on the basis of 18-8CrNi, also known as controlled phase transformation stainless steel. After solution treatment, it is an unstable austenite structure, which has good ductility and processability. After adjustment, the austenite precipitation and carbonization phenology components change, and then through martensitic transformation treatment, most of the structure is transformed into toughness. Better low-carbon tempered martensite, this state is the use state of steel, and has good mechanical properties at medium temperature. Corrosion resistance is better than general martensitic stainless steel.

Aisi 631 / 17-7PH alloy is characterized by heat treatment to obtain high hardness and high strength, excellent fatigue resistance, good corrosion resistance and small heat treatment deformation.

The formability and elasticity of the annealed 17-7PH are similar to those of 301.

Under the heat treatment conditions of TH1050 and RH950, the corrosion resistance of 631 is better than that of general hardenable stainless steel (such as 410, 420 and 431), but not as good as 304. After CH900 heat treatment, its corrosion resistance is similar to that of 304 in most environments.

Like 17-4PH (630), the recommended operating temperature of 631 is below 300°C. Its welding performance is weaker than 630.

Aisi 631 Grade comparison

Chinese

GB

07Cr17Ni7Al

(0Cr17Ni7Al)

USA

ASTM

631

UNS

S17700

AK Steel

17-7 PH®

Japan

JIS

SUS 631

Germany

DIN

X7CrNi17-7

W.Nr.

1.4568

Aisi 631 chemical composition(wt%)

Standard

GB/T 1220-2007

ASTM A693

Grade

07Cr17Ni7Al

UNS S17700

C

≤0.09

≤0.09

Si

≤1.00

≤1.00

Mn

≤1.00

≤1.00

P

≤0.040

≤0.040

S

≤0.030

≤0.030

Cr

16.00~18.00

16.00~18.00

Ni

6.50~7.75

6.50~7.75

Al

0.75~1.50

0.75~1.50

 

 

 

S17700 17-7 PH AISI 631 Stainless Steel Bar 6 Mm Ch 900 Condition Heat Treatment 0S17700 17-7 PH AISI 631 Stainless Steel Bar 6 Mm Ch 900 Condition Heat Treatment 1

Hot Tags: s17700 17-7 ph aisi 631 stainless steel bar 6 mm ch 900 condition heat treatment, China s17700 17-7 ph aisi 631 stainless steel bar 6 mm ch 900 condition heat treatment suppliers, 304 316 Steel Flat Bars With Holes, Stainless Steel 446 Round Bar, 304 304L 316 316L Stainless Round Bar, 420 Stainless H type Steel, Stainless Steel 310S Round Bar

Send Inquiry

whatsapp

Phone

E-mail

Inquiry