S45C 1045 C45 Carbon Steel Bar
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of s45c 1045 c45 carbon steel bar in China. If you're going to wholesale high quality s45c 1045 c45 carbon steel bar made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
S45C 1045 C45 Carbon Steel Bar
Product Introduction
| Steel Grade: | Ss400 A36 S45c Sae1045 42CrMo | Alloy Or Not: | Non-alloy |
|---|---|---|---|
| Technique: | Cold Drawn | Application: | Structural Steel Bar |
| Type: | Carbon Steel Bar | Standard: | ASTM,DIN,GB,AISI,JIS |
| Shape: | Round | Length: | 1--12m |
| Surface: | Black Or Bright | Dimensions: | Dia 8-60mm |
| Heat Treatment: | Normalized +Annealed +Quenched + Tempered | ||
| High Light: |
45# steel round bar,astm steel round bar,sae1045 cold drawn round bar |
||
AISI 1045 steel is a high-strength, high-quality medium carbon steel. It can also be called JIS S45C and DIN C45 steel. Due to poor hardenability, it is usually used in the normalized state. Quenching and tempering treatment is required to obtain higher mechanical properties. Used to manufacture mechanical parts with high strength requirements. Such as gears, shafts, piston pins, etc. The properties and heat treatment of 1045 steel round steel plates are as follows.
1045 steel physical properties
Properties Metric Imperial Density 7.87 g/ml 0.284 lb/in³
C45 steel mechanical properties
Mechanical Properties Metric Imperial Hardness, Brinell 163163, Knoop (converted from Brinell) 184184 Hardness, Rockwell B (converted from Brinell) 8484 Hardness, Vickers (converted from Brinell) Come) 170170 tensile strength, ultimate 565 MPa 81900 psi tensile strength, yield 310 MPa 45000 psi
C45 steel properties
1. It is carbon steel with good weldability and machinability.
2. After normalizing and hot rolling, it has high strength and impact properties.
3. The hardenability is low, and the critical hardenability diameter in water is 12-17mm. And there is a tendency to crack during water quenching.
4. Both hydrogen welding and argon arc welding are good, but gas welding is not. Preheating is required before welding, and stress relief annealing should be performed after welding.
C45 steel application
1045 steel is widely used in industrial applications that require higher strength and wear resistance than mild steel. Typical applications are gears, shafts, rollers, crankshafts, sleeves, bolts, etc.