S32654 1.4652 Stainless Steel Bar Corrosion Resistance Ultra 654 SMO OD 80mm
video

S32654 1.4652 Stainless Steel Bar Corrosion Resistance Ultra 654 SMO OD 80mm

654SMo (S32654, 1.4652) super austenitic stainless steel is a super austenitic stainless steel containing 23% nickel, 25% chromium and 7% molybdenum, its corrosion resistance is much better than ordinary austenitic steel. 654SMo (S32654, 1.4652) super austenitic stainless steel contains high molybdenum. When processing seamless pipe perforations, the steel type is hard and sticky, and it is easy to eccentric or crack. There is a great risk in perforation. The round steel center is perforated and then pierced, and the rolling mill is cold rolled or cold drawn. Although the cost is increased, it can guarantee a high success rate. 654SMo (S32654, 1.4652) super austenitic stainless steel has very good local corrosion resistance. It has good pitting corrosion resistance and good stress corrosion resistance under seawater, aeration, gaps, and low-speed erosion conditions. Alternative materials for nickel-based alloys and titanium alloys. Secondly, in terms of high temperature resistance or corrosion resistance, it has more excellent high temperature resistance or corrosion resistance than 904L and 254SMO.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of s32654 1.4652 stainless steel bar corrosion resistance ultra 654 smo od 80mm in China. If you're going to wholesale high quality s32654 1.4652 stainless steel bar corrosion resistance ultra 654 smo od 80mm made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

S32654 1.4652 Stainless Steel Bar Corrosion Resistance Ultra 654 SMO OD 80mm

Description

Certification: ISO,BV,SGS Type: Round
Application: Construction,decoration,Industry,Mechineal,shipbuilding Standard: ASTM,AISI,JIS,EN
Grade: S32654 1.4652 654SMO Shape: Round
Dimensions: 3mm-800mm Surface: Bright,Polished,black
Technique: Cold Drawn&hot Rolled Length: Customers' Requirements
Packing: Standard Seaworthy Package Price Term: CIF CFR FOB Ex-Work
High Light:

Stainless Steel Bar Corrosion Resistance

,

Stainless Steel 1.4652 Bar

,

Stainless Steel Bar 80mm

S32654 1.4652 654SMO Stainless Steel Bar Corrosion Resistance Ultra 654 SMO OD 80mm

 

Product Description

32652 UNS 654SMO Super Austenitic Stainless Steel 1.4652 X1CrNiMOCUN24-22-8

S32652(UNS 654SMO)Super Austenitic Stainless Steel pipe 1.4652 / X1CrNiMOCUN24-22-8

ASTM A312, ASTM A269 ,S32652 UNS 654SMO 1.4652 X1CrNiMOCUN24-22-8 Super Austenitic Stainless Steel

Product Description

32652 UNS 654SMO Super Austenitic Stainless Steel 1.4652 X1CrNiMOCUN24-22-8

S32652(UNS 654SMO)Super Austenitic Stainless Steel pipe 1.4652 / X1CrNiMOCUN24-22-8

Material Description:

654SMo (S32654, 1.4652) super austenitic stainless steel is a super austenitic stainless steel containing 23% nickel, 25% chromium and 7% molybdenum, its corrosion resistance is much better than ordinary austenitic steel.

654SMo (S32654, 1.4652) super austenitic stainless steel contains high molybdenum. When processing seamless pipe perforations, the steel type is hard and sticky, and it is easy to eccentric or crack. There is a great risk in perforation. The round steel center is perforated and then pierced, and the rolling mill is cold rolled or cold drawn. Although the cost is increased, it can guarantee a high success rate.

654SMo (S32654, 1.4652) super austenitic stainless steel has very good local corrosion resistance. It has good pitting corrosion resistance and good stress corrosion resistance under seawater, aeration, gaps, and low-speed erosion conditions. Alternative materials for nickel-based alloys and titanium alloys. Secondly, in terms of high temperature resistance or corrosion resistance, it has more excellent high temperature resistance or corrosion resistance than 904L and 254SMO.

Description:

S32652 UNS 654SMO 1.4652 X1CrNiMOCUN24-22-8 Super Austenitic Stainless Steel Pipe and Tube

Standard:

ASTM A312 Seamless and Welded Austenitic Stainless Steel Pipe
ASTM A269 Seamless and Welded Austenitic Stainless Steel Pipe for General Equipment
ASTM B673, ASTM B674, ASTM B677, ASTM B675, ASTM B676, ASTM B690

Material: S32652 UNS 654SMO 1.4652 X1CrNiMOCUN24-22-8

Main chemical composition:

C:≤0.02
Si:≤0.05
Mn:2.00-4.00
Ni:21.0-23.0
P:≤0.03
S:≤0.005
Cr:23-25
Mo:7.0-8.0
N:0.45 - 0.55
Cu:0.3-0.6

Performance characteristics:
1. Excellent pitting and crevice corrosion resistance in harsh corrosive environments
2. Excellent mechanical properties and high yield strength
3. Good processability

Size Range for tubing:

OD:1/4" (6.25mm) to 8" (203mm)
WT 0.02" (0.5mm) to 0.5"(12mm)
Length:15m(Max) or as your requirement

Process:
Cold drawn, Cold rolled, Precision Rolled for Seamless Pipe or Tube
Gas tungsten arc welding, Plasma arc welding (PAW),Submerged arc welding (SAW) For Welded Pipe or Tube

Finish: Annealed & pickled, bright annealing, polished

Ends: Beveled or plain end, square cut, burr free ,Plastic Cap at Both end

Packing: Bare packing/bundle packing with woven bag/wooden or steel frame crate packing/plastic cap protection at the both sides of tubes and suitably protected for sea-worthly delivery or as requested.

Inspection and Test Procedure
1. 100% PMI,Spectro Chemical Aanlysis Test for Raw Material
2. 100% Dimension & Visual Examination
3. Mechanical Properties Test Include Tension Test,Flaring Test (For Seamless tube/pipe)/ Flange Test (For Welded Pipe & Tube), Hardness Test ,Reversed Flattening Test
4. 100% Hydrostatic Test or 100% NON-DESTRUCTIVE Test (ET or UT)
5. Radiographic Test for Welded Pipe (shall be accordance with specification,or shall be as agreed upon between the purchaser and vendor)
6. Straightness Test (optional)
7. Roughness Test (optional)
8. Intergranular Corrosion Test(optional)
9. Impact Test (optional)
10. Grain Size Determinations (optional)
NOTES : ALL THE TESTS AND INSPECTION RESULT NEED TO BE SHOWED IN REPORTS ACCORDING TO STANDARD AND SPECIFICATION.

and Tube

Material Description:

654SMo (S32654, 1.4652) super austenitic stainless steel is a super austenitic stainless steel containing 23% nickel, 25% chromium and 7% molybdenum, its corrosion resistance is much better than ordinary austenitic steel.

654SMo (S32654, 1.4652) super austenitic stainless steel contains high molybdenum. When processing seamless pipe perforations, the steel type is hard and sticky, and it is easy to eccentric or crack. There is a great risk in perforation. The round steel center is perforated and then pierced, and the rolling mill is cold rolled or cold drawn. Although the cost is increased, it can guarantee a high success rate.

654SMo (S32654, 1.4652) super austenitic stainless steel has very good local corrosion resistance. It has good pitting corrosion resistance and good stress corrosion resistance under seawater, aeration, gaps, and low-speed erosion conditions. Alternative materials for nickel-based alloys and titanium alloys. Secondly, in terms of high temperature resistance or corrosion resistance, it has more excellent high temperature resistance or corrosion resistance than 904L and 254SMO.

Description:

S32652 UNS 654SMO 1.4652 X1CrNiMOCUN24-22-8 Super Austenitic Stainless Steel Bar

 

Material: S32652 UNS 654SMO 1.4652 X1CrNiMOCUN24-22-8

Main chemical composition:

C:≤0.02
Si:≤0.05
Mn:2.00-4.00
Ni:21.0-23.0
P:≤0.03
S:≤0.005
Cr:23-25
Mo:7.0-8.0
N:0.45 - 0.55
Cu:0.3-0.6

Performance characteristics:
1. Excellent pitting and crevice corrosion resistance in harsh corrosive environments
2. Excellent mechanical properties and high yield strength
3. Good processability

Size Range for tubing:

OD:1/4" (6.25mm) to 8" (203mm)
WT 0.02" (0.5mm) to 0.5"(12mm)
Length:15m(Max) or as your requirement

Process:
Cold drawn, Cold rolled, Precision Rolled for Seamless Pipe or Tube
Gas tungsten arc welding, Plasma arc welding (PAW),Submerged arc welding (SAW) For Welded Pipe or Tube

Finish: Annealed & pickled, bright annealing, polished

Ends: Beveled or plain end, square cut, burr free ,Plastic Cap at Both end

Packing: Bare packing/bundle packing with woven bag/wooden or steel frame crate packing/plastic cap protection at the both sides of tubes and suitably protected for sea-worthly delivery or as requested.

Inspection and Test Procedure
1. 100% PMI,Spectro Chemical Aanlysis Test for Raw Material
2. 100% Dimension & Visual Examination
3. Mechanical Properties Test Include Tension Test,Flaring Test (For Seamless tube/pipe)/ Flange Test (For Welded Pipe & Tube), Hardness Test ,Reversed Flattening Test
4. 100% Hydrostatic Test or 100% NON-DESTRUCTIVE Test (ET or UT)
5. Radiographic Test for Welded Pipe (shall be accordance with specification,or shall be as agreed upon between the purchaser and vendor)
6. Straightness Test (optional)
7. Roughness Test (optional)
8. Intergranular Corrosion Test(optional)
9. Impact Test (optional)
10. Grain Size Determinations (optional)
NOTES : ALL THE TESTS AND INSPECTION RESULT NEED TO BE SHOWED IN REPORTS ACCORDING TO STANDARD AND SPECIFICATION.

S32654  1.4652 Stainless Steel Bar Corrosion Resistance Ultra 654 SMO OD 80mm 0

S32654  1.4652 Stainless Steel Bar Corrosion Resistance Ultra 654 SMO OD 80mm 1

Hot Tags: s32654 1.4652 stainless steel bar corrosion resistance ultra 654 smo od 80mm, China s32654 1.4652 stainless steel bar corrosion resistance ultra 654 smo od 80mm suppliers, 304 316 Steel Flat Bars With Holes, Stainless Steel 310S Round Bar, 420 Stainless H type Steel, Stainless Steel 446 Round Bar, 304 304L 316 316L Stainless Round Bar

Send Inquiry

whatsapp

Phone

E-mail

Inquiry