EN 1.7131 80mm Steel Bar 16mncr5H Steel 16mncr5 Tensile Strength SAE 51204 Equivalent
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of en 1.7131 80mm steel bar 16mncr5h steel 16mncr5 tensile strength sae 51204 equivalent in China. If you're going to wholesale high quality en 1.7131 80mm steel bar 16mncr5h steel 16mncr5 tensile strength sae 51204 equivalent made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
EN 1.7131 80mm Steel Bar 16mncr5H Steel 16mncr5 Tensile Strength SAE 51204 Equivalent
Description
| OD: | 6-400MM | Length: | 5800 6000mm 9000mm |
|---|---|---|---|
| Surface: | Black | Standard: | GB ASTM |
| DIN Standard: | EN 10084 : 2008 | Condition: | End Quenchh Test Quenching |
| High Light: |
forged steel round bar,carbon steel round bars |
||
16MnCr5,16MnCr5 Chemical composition,16MnCr5 steel grades,if you need EN 10084 : 2008 Case hardening steels. Technical delivery conditions ,please contact us.
| Grade : | 16MnCr5 |
| Number: | 1.7131 |
| Standard: | EN 10084 : 2008 Case hardening steels. Technical delivery conditions EN 10132 - 2 : 2000 Cold rolled narrow steel strip for heat treatment. Technical delivery conditions. Case hardening steels |
| Classification: | Case hardening steels |
| Equivalent grades: | Go here |
| 16MnCr5 EN 10084-1998, Number: 1.7131 | Comparison of steel grades | |
| JUS | Č.4320 | |
| DIN | 16MnCr 5; ZF 6 | |
| BS | 590M17, | |
| GOST | 18HG | |
| AISI | SAE 5115, SAE 51204 | |
| UNI | 16MnCr5 | |
| NF | 16MC5 | |
Chemical composition (cast analysis)
| Chemical elements | C | Si max. |
Mn | P max. | S | Cr |
| %, by mass | 0,14-0,19 | 0,40 | 1,00-1,30 | 0,035 | ≤ 0,035 | 0,80 – 1,10 |
| Permissible deviation | ± 0,02 | + 0,03 | ± 0,05 | + 0,005 | + 0,005 | ± 0,05 |
Hardness limits for steel
| Hardness HRC at a distance from quenched end of test piece (in milimetres) of | ||||||||||||||||
| mm | 1,5 | 3 | 5 | 7 | 9 | 11 | 13 | 15 | 20 | 25 | 30 | 35 | 40 | 45 | 50 | |
| +H | max. | 47 | 46 | 44 | 41 | 39 | 37 | 35 | 33 | 31 | 30 | 29 | 28 | 27 | - | - |
| min. | 39 | 36 | 31 | 28 | 24 | 21 | - | - | - | - | - | - | - | - | - | |
| +HH | max. | 47 | 46 | 44 | 41 | 39 | 37 | 35 | 33 | 31 | 30 | 29 | 28 | 27 | - | - |
| min. | 42 | 39 | 35 | 32 | 29 | 26 | 24 | 22 | 20 | - | - | - | - | - | - | |
| +HL | max. | 44 | 43 | 40 | 37 | 34 | 32 | 30 | 28 | 26 | 25 | 24 | 23 | 22 | - | - |
| min. | 39 | 36 | 31 | 28 | 24 | 21 | - | - | - | - | - | - | - | - | - | |
Hardness requirements for products delivered in the conditions ''treated to improve shearabilita'' (+S), ''anneled to maximum hardness requirements'' (+A), ''treated to hardness range'' (+TH) or ''treated to ferrite-pearlite structure and hardness range'' (+FP)
| Brinell hardness in the condition | ||||||
| +S max. | +A max. | +TH | +FP | |||
| min. | max. | min. | max. | |||
| * | 207 | 156 | 207 | 140 | 187 | |
Non-metallic inclusions Requirements for microscopic degree of purity when tested in accordance with DIN 50 602 (method K) (valid for oxidic non-metallic inclusions)
| D (mm) Bars Diameter d (mm) | K Total characteristic value K (oxides) for the individual cast |
| 140 < d 200 | K 4 ≤ 50 |
| 100 < d ≤ 140 | K 4 ≤ 45 |
| 70 < d ≤ 100 | K 4 ≤ 40 |
| 35 < d ≤ 70 | K 4 ≤ 35 |
| 17 < d ≤ 35 | K 3 ≤ 40 |
| 8 < d ≤ 17 | K 3 ≤ 30 |
| d ≤ 8 | K 2≤ 35 |
Conditions for heat treating test bars and treatment of the steels
| End quenchh test Quenching, 0C | Carbunnzing temperature, 0C | Core-hardening temperature, 0C | Case-hardening temperature, 0C | Tempering, 0C |
| 870 | 880 to 980 | 860 to 900 | 780 to 820 | 150 to 200 |





Hot Tags: en 1.7131 80mm steel bar 16mncr5h steel 16mncr5 tensile strength sae 51204 equivalent, China en 1.7131 80mm steel bar 16mncr5h steel 16mncr5 tensile strength sae 51204 equivalent suppliers, Stainless Steel 310S Round Bar, 304 316 Steel Flat Bars With Holes, Stainless Steel 446 Round Bar, 304 304L 316 316L Stainless Round Bar, 420 Stainless H type Steel