DUPLEX WELDED 2507 Stainless Steel Welded Pipe, FULL FINISHED AND BRIGHT ANNEALED, SMOOTH ENDS, FREE OF BURRS
video

DUPLEX WELDED 2507 Stainless Steel Welded Pipe, FULL FINISHED AND BRIGHT ANNEALED, SMOOTH ENDS, FREE OF BURRS

Duplex Stainless Steel have a structure that contains both ferrite and austenite. Duplex alloys have higher strength and better stress corrosion cracking resistance than most austenitic alloys and greater toughness than ferritic alloys, especially at low temperatures. The corrosion resistance of duplex alloys depends primarily on their composition, especially the amount of chromium, molybdenum, and nitrogen they contain.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of duplex welded 2507 stainless steel welded pipe, full finished and bright annealed, smooth ends, free of burrs in China. If you're going to wholesale high quality duplex welded 2507 stainless steel welded pipe, full finished and bright annealed, smooth ends, free of burrs made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

DUPLEX WELDED 2507 Stainless Steel Welded Pipe, FULL FINISHED AND BRIGHT ANNEALED, SMOOTH ENDS, FREE OF BURRS

Description

Length: 6-11meter OD: 10-325mm
Thickness: SCH10 - SCH 160 Technique: Welded
Steel Grade: Duplex Stainless Steel Welding Line Type: ERW
Standard: ASTM,AISI,DIN Application: Construction,Decoration,Industry
Shape: Round.square.Rectangle Surface: Annealing
Thickness: 0.5-25.4mm
High Light:

ss seamless pipes

,

astm stainless steel pipe

Standard: ASTM/ASME A/SA789, A/SA790, A/SA928, DIN17456/17458, EN10216-5. After negotiation, we can supply

pipe with customers'requirement.

Material Grade:

UNS EN DIN C % Cr% Ni% Mo% N% Other %
S31803 1.4462 X2CrNiMoN22-5-3 0.030max 21.0-23.0 4.5-6.5 2.5-3.5 0.08-0.20 /
S32205 1.4462 X2CrNiMoN22-5-3 0.030max 22.0-23.0 4.5-6.5 3.0-3.5 0.14-0.20 /
S32101 1.4162   0.040max 21.0-22.0 1.35-1.70 0.10-0.80 0.20-0.25 Cu 0.10-0.80
S32304     0.030max 21.5-24.5 3.0-5.5 0.05-0.60 0.15-0.20 Cu 0.05-0.60
S32750 1.4410 X2CrNiMoN25-7-4 0.030max 24.0-26.0 6.0-8.0 3.0-5.0 0.24-0.32 Cu 0.50max
S32760     0.050max 24.0-26.0 6.0-8.0 3.0-4.0 0.20-0.30 Cu 0.50-1.00

 

 

Mechanical Property:

 

UNS Tensile Strength
Min, Mpa
Yield Strength
Min, Mpa
Elongation in 2 in Or 50mm Min, % Hardness Max,
HRC
S31803 620 450 25 30
S32205 655 485 25 30
S32101 700 530 30 30
S32304 690 450 25 30
S32750 800 550 15 32
S32760 750 550 25 32

 

Size Range:

 

Stainless Steel Seamless Tube ASTM A789/A789M: OD: Φ12.7mm-Φ203mm; WT:0.5mm-6.35mm
Stainless Steel Welded Tube ASTM A789/A789M: OD: Φ12.7mm-Φ203mm; WT:0.5mm-4.0mm

 

Duplex Stainless Steel have a structure that contains both ferrite and austenite. Duplex alloys have higher strength and better stress corrosion cracking resistance than most austenitic alloys and greater toughness than ferritic alloys, especially at low temperatures. The corrosion resistance of duplex alloys depends primarily on their composition, especially the amount of chromium, molybdenum, and nitrogen they contain.

 

 

Standard: ASTM/ASME A/SA789, A/SA790, A/SA928, DIN17456/17458, EN10216-5. After negotiation, we can supply pipe with customers'requirement.

Material Grade:UNS S31803,S32205,S32101,S32304,S32750,S32760,1.4462,1.4410etc.

Size Range:

 

Stainless Steel Seamless Tube ASTM A789/A789M: OD: Φ12.7mm-Φ203mm; WT:0.5mm-6.35mm
Stainless Steel Seamless Pipe ASTM A790/A790M: OD: Φ6mm-Φ325mm; WT:0.5mm-30mm
Stainless Steel Welded Tube ASTM A789/A789M: OD: Φ12.7mm-Φ203mm; WT:0.5mm-4.0mm

 

Stainless Steel Welded Pipe

ASTM A790/A790M: OD: Φ10mm-Φ2000mm; WT:0.5mm-40mm

(OD≤630mm for single seam; OD>Φ630mm For circumferential seam)

ASTM A928/A928M: OD: Φ10mm-Φ406mm; WT:0.5mm-10mm.

 

Chemical Composition, %

Cr

Ni

Mo

C

N

Mn

24.0-26.0

6.0-8.0

3.0-5.0

0.030 Max

.24-.32

1.20 Max

Si

Cu

P

S

Fe

 

0.80 Max

0.50 Max

0.035 Max

0.020 Max

Balance

 

In what applications is Duplex 2507 used?

Desalination Equipment

Chemical process pressure vessels, piping and heat exchangers

Marine Applications

Flue Gas Scrubbing Equipment

Pulp & Paper Mill Equipment

Offshore Oil production/technology

Oil and gas industry equipment

ASTM Specifications

Pipe Smls

Pipe Welded

Tube Smls

Tube Welded

Sheet/Plate

Bar

Flanges & Fittings

A790

A790

A789

A789

A240

A276

A182

Mechanical Properties
Specified Tensile Properties, Plate ASTM A240

Ultimate Tensile Strength, ksi Minimum

.2% Yield Strength, ksi Minimum

% Elongation Min.

 

116

80

15

310

Company Information---The Reason Why You Will Choose Us

We are an large storage company and have our own factory . We specialize in stainless steel products for 23 years, we can supply Processing services , including cutting ,welding , surface treatment and precision processing.

Our product line includes stainless steel sheet/plate/circle/coil/strip/pipe/tube/bar. etc and galvanized steel sheet/plate/coil/strip. etc . More than 200 kinds of products for your choice .

We can also supply special stainless steel product , such as Monel / Incoloy / Inconel / Hastelloy .etc

we have strict inspection system to ensure the quality, and all processes are carried out according to ISO 9001: 2008.

we are nominated as the AAA enterprise by Jiangsu government.

We are powerful manufacturer audited by world top inspection company ISO ,SGS, TUV and BV.

Our products have been exported to more than 60 countries and regions, including Europe, Middle East, South Asia, South America, Africa, United Arab Emirates .etc.

The annual production capacity is 50000 tons stainless steel products.

 

 

DUPLEX WELDED 2507 Stainless Steel Welded Pipe, FULL FINISHED AND BRIGHT ANNEALED, SMOOTH ENDS, FREE OF BURRS 0DUPLEX WELDED 2507 Stainless Steel Welded Pipe, FULL FINISHED AND BRIGHT ANNEALED, SMOOTH ENDS, FREE OF BURRS 1DUPLEX WELDED 2507 Stainless Steel Welded Pipe, FULL FINISHED AND BRIGHT ANNEALED, SMOOTH ENDS, FREE OF BURRS 2

 

FAQ

Q:What is your competitive advantage ?

A: We have many professional technical personnel.And we have more competitive prices and better after-sales service .

 

Q:How do you control the quality?

A:Our company is certificated to ISO9001:2008.We have many inspectors and every product will have been tested for 4-5 processes.

We welcome customers or the third party inspection agencies to come to our factory for inspection.

 

Q:What about your price?

A:Our price is very competitive because we are a factory.

 

Q:How long is your delivery time?

A:Different products have different delivery time.The products will be delivered as soon as possible on the basis of the quality assurance.Usually the delivery time is within 5-10 days after we receive your deposit.

 

Q:Do you have a published price list?

A:We do NOT have a published price list. In our business market, conditions are always fluctuating, which makes standard pricing difficult to maintain. We allow our sales staff to be flexible when it comes to quoting on your requirements, which means that you will receive the best price available when you need it.

Hot Tags: duplex welded 2507 stainless steel welded pipe, full finished and bright annealed, smooth ends, free of burrs, China duplex welded 2507 stainless steel welded pipe, full finished and bright annealed, smooth ends, free of burrs suppliers, 304 316 Steel Flat Bars With Holes, Stainless Steel 310S Round Bar, 420 Stainless H type Steel, 304 304L 316 316L Stainless Round Bar, Stainless Steel 446 Round Bar

Send Inquiry

whatsapp

Phone

E-mail

Inquiry