Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of din 1.4539 904l stainless round bar in China. If you're going to wholesale high quality din 1.4539 904l stainless round bar made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Stainless Steel 1.4539 Bar Introduction:
1.4539 904L stainless steel bar combines molybdenum and copper with iron for tremendously increased resistance to reducing acids like sulphuric acid. It stands up extremely well to chlorides in the environment for low pitting and crevice corrosion, as well as stress corrosion cracking.
1.4539 SS Round Bar Applications:
1.4539 904L Round Bar is widely used in the chemical, pharmaceutical, oil and gas industries. Typical applications include tanks, valves, heat exchangers, flanges and manifolds. The addition of copper to the composition of 904L ss round bar aids its suitability for components such as tanks and other products used in handling sulphuric and phosphoric acid.

SS 1.4539 Pipe Modulus Temperature Range
| TEMPERATURE, °C | J/(KG °C) | TEMPERATURE, °F | BTU/(LB °F) |
|---|---|---|---|
| 20 | 460 | 68 | 0.11 |
| 100 | 485 | 200 | 0.12 |
| 200 | 515 | 400 | 0.12 |
| 300 | 545 | 600 | 0.13 |
| 400 | 570 | 800 | 0.14 |
| 500 | 590 | 1000 | 0.14 |
| 600 | 605 | 1200 | 0.15 |
| 700 | 615 | 1300 | 0.15 |
1.4539 Chemical Composition(%):
| Steel Grade | C | Si | Mn | P | S | Cr | Ni | Mo | Cu | N |
|---|---|---|---|---|---|---|---|---|---|---|
| 904L | 0.02 max | 1.0 max | 2.0 max | 0.040 max | 0.030 max | 19.0-23.0 | 23.0-28.0 | 4.0-5.0 | 1.0-2.0 | 0.10 max |
| 1.4539 | 0.02 max | 0.7 max | 2.0 max | 0.040 max | 0.010 max | 19.0-21.0 | 24.0-26.0 | 4.0-5.0 | 1.2-2.0 | 0.15 max |
DIN 1.4539 Mechanical Properties (Annealed):
| Hardness (HB) | Tensile Strength (Mpa) | Yield Strength (Mpa) | Elongation (%) (Long.) | Impact Value (J) (Long.) |
|---|---|---|---|---|
| 230 max | 530-730 | 230-260 | 35 min | 100 min |
Customer Visit

The Group adheres to the tenet of "one-stop service, making choices easier" and adheres to the business philosophy of "successful customers, happy employees; embracing change, the most important thing is action", and continues to meet the different needs of global customers in the field of the world's steel supply chain. need. A professional sales team provides customers with first-class services; a strict procurement and quality inspection team carefully selects high-quality raw materials; an advanced science and technology team improves production and reduces costs for customers; an excellent design and processing team strives for excellence. Considerate shipping and logistics team to protect product transportation.
Hot Tags: din 1.4539 904l stainless round bar, China din 1.4539 904l stainless round bar suppliers, Stainless Steel 310S Round Bar, Stainless Steel 446 Round Bar, 304 316 Steel Flat Bars With Holes, 304 304L 316 316L Stainless Round Bar, 420 Stainless H type Steel
You Might Also Like
Send Inquiry