AISI310 Stainless Steel Rod
video

AISI310 Stainless Steel Rod

310 grade, is produced for heat resistance purposes. In normal conditions this grade is resistant up to 1100 °C degrees. In the oxidising conditions, when the heat is constant maximum heat resistance can reach 1100 °C degrees, but if the heating is scattered thisgrade is recommenended up to 1030 °C degrees.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of aisi310 stainless steel rod in China. If you're going to wholesale high quality aisi310 stainless steel rod made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

310 grade, is produced for heat resistance purposes. In normal conditions this grade is resistant up to 1100 °C degrees.

In the oxidising conditions, when the heat is constant maximum heat resistance can reach 1100 °C degrees, but if the heating is scattered thisgrade is recommenended up to 1030 °C degrees.

310S grade, is resistant to heat in both dry and moist environments. Due to lower Carbon (C) content, 310S grade has higher resistance to heat than 310. Also with its high Chromium (Cr) content, they also have good corrosion resistance in moist enviornments. Under normal conditions their corrosion resistance is great.

181

Grade
(AISI)

Tensile Strength
(MPa) min

Yield Strength
0.2% Proof
(MPa) min

Elongation
(% in 50mm)
min

Hardness

Rockwell
B (HRB) max

Brinell
(HB) max

310S

515

205

40

95

217

Grade
(AISI)

Density
(kg/m3)

Modulus of
Elasticity

(GPa)

Coeff. of
Thermal Exp.
(mm/m/°C)

Specific Thermal
Capacity
(W/m.K)

Specific Heat
0-100°C
(J/kg.K)

Electrical
Resistivity
(nW.m)

0-100
°C

0-315
°C

0-538
°C

At
100°C

At
500°C

310S

7750

200

15.9

16.2

17.0

14.2

18.7

500

720

Hot Tags: aisi310 stainless steel rod, China aisi310 stainless steel rod suppliers, 304 316 Steel Flat Bars With Holes, 304 304L 316 316L Stainless Round Bar, Stainless Steel 446 Round Bar, Stainless Steel 310S Round Bar, 420 Stainless H type Steel