AISI 321 Stainless Steel Rod
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of aisi 321 stainless steel rod in China. If you're going to wholesale high quality aisi 321 stainless steel rod made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
321 grade is within austenitic stainless steels group, and is stabilised with Titanium (Ti).
Corrosion resistance is similar to 304L grade, and it is resistant to natural waters. Intergranular corrosion resistance is superior due to Titanium (Ti) addition.
Formability and weldability is good in 321 grade, similar to other austenitic grades. Machinability and forgability is low. Heat resistance is up to 900°C.
This grade is non magnetic in annealed condition. 321 grade is not polishable, therefore not suitable for decorative purposes.

|
Grade |
C |
Mn |
Si |
P |
S |
Cr |
Mo |
Ni |
Ti |
|
|
321 |
min. max. |
- 0.08 |
- 2.0 |
- 1.0 |
- 0.045 |
- 0.015 |
17.0 19.0 |
- |
9.0 12.5 |
- 0.70 |
Key Features of 439 Aluminized Stainless Steel Plate
Corrosion Resistance: The aluminized coating provides superior resistance to oxidation and atmospheric corrosion.
High-Temperature Stability: Maintains structural integrity and resists scaling at elevated temperatures.
Weldability: Good weldability, compatible with various welding processes.
Formability: Excellent formability, allowing for easy fabrication of complex shapes.
Heat Reflectivity: The aluminized surface reflects heat, making it ideal for applications requiring thermal management.
Cost-Effective: Provides a cost-effective solution for high-temperature and corrosive environments.
Hot Tags: aisi 321 stainless steel rod, China aisi 321 stainless steel rod suppliers, 304 304L 316 316L Stainless Round Bar, 304 316 Steel Flat Bars With Holes, 420 Stainless H type Steel, Stainless Steel 446 Round Bar, Stainless Steel 310S Round Bar