Stainless Steel 430 Sheets And Plates
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of stainless steel 430 sheets and plates in China. If you're going to wholesale high quality stainless steel 430 sheets and plates made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
These SS 430 Sheets & Plates are the very popular grade of stainless steel due to its features. These plates are designed in such a way to meet all your diverse needs. These plates are available in different sizes and diameter and thickness as per the customer's specifications and needs. These sheets and plates are non-hardenable and contain straight chromium and belong to the ferritic groups of steel. These sheets and plates have good corrosion resistance and formality properties which make it a great choice for the mechanical industry.




It is used widely used due to its high heat resistance property it is less expensive than chromium and nickel grades. These SS sheets and plates are known for service in reducing and oxidizing environments. These sheets are resistant to harsh concentration chemicals and organic and inorganic compounds.
The SS 430 Sheets & Plates are used in many applications such as machine building. Pylons and other architectural structures, construction of bridges, framework structures, truck frames, rail and car parts, making containers, vehicles and transport equipment, in steel constructions. These plates and sheets are also used in security doors and tumbling machines.
These sheets and plates are used in different industries for various applications. it is used in applications such as household appliances, metal molding trim, cabinet hardware, hinges and so on. These plates are ideal for the application of where sanitation is critical or where there is a constant risk of corrosion. It does not get rust, and so it does not need protection from moisture or chemicals. It does not any painting or polishing and does not lose its color very easily.
We have many years of experience with SS plates. We make several types of tests to provide the best products. We even test the raw material before the formation so that there will be no possible chances of any type of error. We also provide all the documentation of the tests followed.
430 STAINLESS STEEL SHEETS AND PLATES EQUIVALENT GRADES
| STANDARD | UNS | WNR. |
|---|---|---|
| SS 430 | S43000 | 1.4016 |
Stainless Steel Sheets and Plates Specification : ASTM A240 / ASME SA240
Dimension Standard : JIS, AISI, ASTM, GB, DIN, EN, etc
Width : 1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm, etc
Length : 2000mm, 2440mm, 3000mm, 5800mm, 6000mm, etc
Thickness : 0.3 mm to 120 mm
Form : Coils, Foils, Rolls, Plain Sheet, Shim Sheet, Perforated Sheet, Chequered Plate, Strip, Flats, Blank (Circle), Ring (Flange) etc.
Surface Finishing : Hot rolled plate (HR), Cold rolled sheet (CR),2B, 2D, BA, NO.1, NO.4, NO.8, 8K, mirror, Chequered, embossed, hair line, sand blast, Brush, etching, SATIN (Met with Plastic Coated) etc.
CHEMICAL COMPOSITION OF STAINLESS STEEL 430 SHEETS AND PLATES
| Grade | C | Mn | Si | P | S | Cr | Ni |
|---|---|---|---|---|---|---|---|
| 430 | 0.12 max | 1.00 max | 1.00 max | 0.040 max | 0.030 max | 16.0 - 18.0 | 0.75 max |
MECHANICAL PROPERTIES OF STAINLESS STEEL 430 SHEETS AND PLATES
| Tensile Strength (MPa) min | Yield Strength 0.2% Proof (MPa) min | Elongation (% in 50mm) min | Hardness | |
|---|---|---|---|---|
| Rockwell B (HR B) max | Brinell (HB) max | |||
| 450 | 205 | 22 | 89 | 183 |
FAQ
Q: How do you control quality ?
A: Mill Test Certification is supplied with shipment, Third Party Inspection is available. and we also get ISO,SGS,Alibaba Verified.
Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.
Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.
Q: Can you provide sample ?
A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.
Hot Tags: stainless steel 430 sheets and plates, China stainless steel 430 sheets and plates suppliers, SS410 Stainless Steel Plate, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, Corrugated SS Roof Sheet, ASTM A240 Grade 431 10mm Stainless Steel Plate, 1 4510 Stainless Steel Patterned Plate, Stainless Steel 316 316L 316Ti Sheets And Plates
You Might Also Like
Send Inquiry