Stainless 316 Steel Plate
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of stainless 316 steel plate in China. If you're going to wholesale high quality stainless 316 steel plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
1. Thickness range:
Thin plates: Thickness is usually between 0.3mm and 3mm.
Medium plates: Thickness is between 3mm and 20mm.
Thick plates: Thickness is over 20mm, often used for heavy industrial purposes.

2. Width and length:
Common widths: 1000mm, 1219mm (4 feet), 1500mm, 1800mm, etc.
Common lengths: 2000mm, 2438mm (8 feet), 3000mm, 6000mm.
Coils: Stainless steel coils can also be supplied, and the width and thickness can be customized according to requirements.
3. Surface treatment:
2B surface: Commonly used in industrial applications, matte, smooth surface.
BA surface: Bright surface treatment, often used for decorative purposes.
No. 4 surface: Brushed treatment, suitable for architectural decoration.
No. 1 surface: Surface treatment after hot rolling, usually rough, suitable for structural applications.

4. Mechanical properties:
Tensile strength: 515-1035 MPa.
Yield strength: 205 MPa (minimum).
Elongation: 40%.
5. Standard size:
Conforms to ASTM A240, which is a common international standard for stainless steel plates.
There are also different regional standards such as JIS and EN.
6. Processing form:
316 stainless steel plates can be processed by shearing, bending, laser cutting, etc. according to needs to meet different manufacturing needs.
Hot Tags: stainless 316 steel plate, China stainless 316 steel plate suppliers, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, Corrugated SS Roof Sheet, 1 4510 Stainless Steel Patterned Plate, SS410 Stainless Steel Plate, SS409 Stainless Steel Welded Pipe, SS431 Stainless Steel Plate