Stainless 301 Steel Plate
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of stainless 301 steel plate in China. If you're going to wholesale high quality stainless 301 steel plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
301 stainless steel plate is a high-strength, corrosion-resistant austenitic stainless steel. It is known for its high work-hardening rate and excellent mechanical properties, making it a versatile material for various demanding applications. Here are some key features and benefits of 301 stainless steel plate:

Composition: 301 stainless steel typically contains 16-18% chromium and 6-8% nickel, along with small amounts of carbon, manganese, silicon, and nitrogen.
| Specification | Details |
|---|---|
| Grade | 301 |
| Standard | ASTM A240, AMS 5517, EN 1.4310 |
| - Thickness | 0.3mm to 6.0mm |
| - Width | 1000mm, 1219mm, 1500mm, custom widths available |
| - Length | 2000mm, 2440mm, 3000mm, 6000mm, custom lengths available |
| Surface Finish | |
| - 2B | Smooth, reflective finish |
| - BA (Bright Annealed) | Highly reflective finish |
| - No. 4 | Brushed finish with a unidirectional texture |
| - No. 1 | Hot rolled, annealed, and pickled finish |
| Certifications | ISO 9001:2015, ASTM, EN, and other international standards |
| Applications | Automotive parts, aerospace components, railway structures, consumer goods, industrial machinery |
Corrosion Resistance: It offers good resistance to corrosion in a variety of environments, although it is less resistant compared to the 304 stainless steel grade.
High Work-Hardening Rate: 301 stainless steel can be significantly strengthened through cold working, making it ideal for applications requiring high strength.
Good Formability: Despite its high strength, it retains good formability, allowing it to be readily formed and fabricated into complex shapes.

301 stainless steel plate is used in a wide range of industries and applications, including:
Automotive Industry: Used for manufacturing parts like springs, trim, and fasteners due to its high strength and resistance to fatigue.
Aerospace Industry: Employed in making aircraft components that require high strength-to-weight ratios and good resistance to corrosion.
Railway Industry: Utilized for making structural components and decorative elements that need both strength and aesthetic appeal.
Consumer Goods: Found in items such as cookware, utensils, and appliances, where durability and resistance to corrosion are important.
Industrial Applications: Used in the manufacturing of conveyor belts, heat exchangers, and other machinery where strength and corrosion resistance are essential.
301 stainless steel plate is a highly versatile material offering a good balance of strength, corrosion resistance, and formability. Its high work-hardening rate and excellent mechanical properties make it suitable for a variety of demanding applications across multiple industries.