SS420 Stainless Steel Plate
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of ss420 stainless steel plate in China. If you're going to wholesale high quality ss420 stainless steel plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
SS 420 grade is widely used in industrial applications due to its good characteristics. The grade contains good quality of vanadium, sulfur, and molybdenum in their composition. Martensitic stainless steels contain high carbon content and manifest right hardness characteristic. Certain steels are frequently fabricated using methods that require hardening and tempering treatments. The operating circumstances of martensitic steels are affected by the loss of material's strength at high temperatures and a decrease in extensibility at negative temperatures. The SS 420 plates exhibits excellent corrosion resistance, oxidation resistance, pitting resistance, good ductility, malleability, and excellent weldability.

| FEATURES OF SS 420 PLATE | DETAILS |
|---|---|
| Standard | ASTM A240 / ASME SA240 |
| Class | SS 420 |
| Dimension | 5mm to 50mm |
| Size (Width) | 1000mm, 1219mm, 1250mm, 1500mm, 2000mm |
| Size (Length) | 2000mm, 2440mm, 2500mm, 3000mm, 6000mm |
SS 420 stainless steel plate is a versatile and high-performance material known for its excellent hardness, strength, and wear resistance. Its ability to withstand moderate corrosive environments makes it ideal for a wide range of applications, from cutlery and medical instruments to industrial tools and automotive parts. With its robust properties and heat treatment capabilities, SS 420 ensures long-lasting performance and reliability in demanding conditions.
Hot Tags: ss420 stainless steel plate, China ss420 stainless steel plate suppliers, 400 2 4360 Alloy Pipe, Corrugated SS Roof Sheet, SS431 Stainless Steel Plate, 1 4510 Stainless Steel Patterned Plate, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, SS409 Stainless Steel Welded Pipe