SS309 Stainless Steel Shim
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of ss309 stainless steel shim in China. If you're going to wholesale high quality ss309 stainless steel shim made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
We manufacture these SS309 Shims with different specifications, shapes, sizes, attributes, and properties to work with different sorts of applications. The surface finish of these SS309 Shims comes in the form of hot rolled and cold rolled.

SS 309 Shims contains a great amount of Stainless steel, and its corrosion resistance and mechanical properties can be further enhanced. It needs to add some other elements, such as nickel, molybdenum, titanium, niobium, manganese. The mechanical components of these SS309 Shims are best as they offer great attributes, cut edgings and strengths to work with different sorts of applications. We manufacture these SS 309 Shims to work with the critical application without any complexity.
| Grade | C | Mn | Si | P | S | Cr | Ni | Fe |
|---|---|---|---|---|---|---|---|---|
| SS 309 | 0.20 max | 2 | 1 | 0.045 max | 0.030 max | 23 max | 14 max | 0 max |

SS 309 Shims are high-alloy irons that allow superior corrosion resistance to other austenitic stainless steel with greater chromium content. These high qualitative Shims are constructed utilizing superior quality raw material compositions provided by our most advanced and trusted vendor in the market. We provide high-quality features with our shims, such as they are adamant, durable, and have satisfactory completion and dimensional exactness. Our SS309 Shims are lightweight mat finish, and we offer grade furnishings that suit the industrial applications criteria.
Our manufactured SS 309 Shims are broadly used and highly demanded in different industries such as various condensers, cooking or kitchen utensils, refrigeration, and air conditioning, restaurant equipment, food packing, oil sectors and many more. We manufacture the SS309 Shims in a way that can perform better with critical applications. Also, they have incredible joining as well as welding properties. The mechanical and physical properties are also better for these SS309 Shims. These shims also contain great adaptability to both cold and hot processing. SS309 Shims also actively reacts to anti-oxidizing.
Hot Tags: ss309 stainless steel shim, China ss309 stainless steel shim suppliers, SS409 Stainless Steel Welded Pipe, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, 1 4510 Stainless Steel Patterned Plate, SS431 Stainless Steel Plate, Stainless Steel 316 316L 316Ti Sheets And Plates, 400 2 4360 Alloy Pipe