904l Stainless Steel Composition N08904 2000mm Length
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 904l stainless steel composition n08904 2000mm length in China. If you're going to wholesale high quality 904l stainless steel composition n08904 2000mm length made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
904L stainless steel combines molybdenum and copper with iron for tremendously increased resistance to reducing acids like sulphuric acid. It stands up extremely well to chlorides in the environment for low pitting and crevice corrosion, as well as stress corrosion cracking.
We can process this steel to fit your applications using our in house processing capabilities and service on your timeline.
Grade 904L stainless steel is one of many stainless steel grades that can be purchased at Tampa Bay Steel.
The "L" in 904L stands for Low Carbon, specifically, that carbon added to the alloy represents .03 percent or less. This means that 904L has very good welding properties. It is also an austenitic alloy, which means that a nonmagnetic solid solution of ferric carbide or carbon in iron is used to increase corrosion resistance.
Properties and Uses of 904L Stainless Steel
904L cannot be hardened by heat treatment. You can weld 904L stainless using any standard method, but it is susceptible to hot cracking. It can be machined but does not machine well.
Common applications take advantage of 904L's corrosion resistance. These include acid processing plants, pulp and paper operations, equipment for cooling seawater, oil refining, and environmental equipment.
The chemical processing industry makes extensive use of 904L stainless steel due to its broad corrosion resistance.
| Grade | Tensile Strength (MPa) min | Yield Strength 0.2% Proof (MPa) min | Elongation (% in 50mm) min | Hardness | |
| Rockwell B (HR B) | Brinell (HB) | ||||
| 904L | 490 | 220 | 36 | 70-90 typical | 150 |




FAQ
Q: Can I get your best price?
A: Our goal is to provide you the best price with great quality assured in a long run. Please leave your contact information for the best quotations, we will get back to you with the best solutions as soon as we can.
Q:What are the shipping ports?
A:Under normal circumstances, we ship from Shanghai, Tianjin, Qingdao, Ningbo ports, you can choose other ports according to your needs.
Q: Why choose us?
A: We are an iron and steel enterprise integrating industry and trade, Our company have been in steel business for more than ten years, we are internationally experienced, professional, and we can provide variety of steel products with high quality to our clients.
Hot Tags: 904l stainless steel composition n08904 2000mm length, China 904l stainless steel composition n08904 2000mm length suppliers, Corrugated SS Roof Sheet, SS410 Stainless Steel Plate, SS409 Stainless Steel Welded Pipe, SS431 Stainless Steel Plate, ASTM A240 Grade 431 10mm Stainless Steel Plate, Stainless Steel 316 316L 316Ti Sheets And Plates
You Might Also Like