440c Stainless Steel 1.4125 UNS S44004
video

440c Stainless Steel 1.4125 UNS S44004

Model NO. 440C Certification ISO Shape Round, Square, Flat Technique Hot Rolled, Forged Surface Treatment Grinded, Peeled, Polished, Rough Turned Similar Grades DIN 1.4125 Uns S44004 Size Range Diameter: 20-480mm Delivery Condition Annealed, Qunched and Tempered Surface Condition Grinded, Peeled, Polished, Rough Turned Quality Standard ASTM-A276
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 440c stainless steel 1.4125 uns s44004 in China. If you're going to wholesale high quality 440c stainless steel 1.4125 uns s44004 made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

440c Stainless Steel (1.4125 UNS S44004)

Product Description

Similar Grades:
DIN 1.4125, S44004, X105CrMo17
Shape:
Round, Flat, Square.
Size Range:

  Diameter(mm) Thickness (mm) Width (mm) Length(mm)
Round 20-480 - - 2000-5800
Square 20-480 - - 2000-5800
flat - 20-50 80-600 2000-5800


Steel-making Condition:
EF, EF/EAF+LF+VD, EF/EAF+ESR
Delivery Condition:
Annealed , Quenched + Tempered

Surface Condition:
Black, Grinded, Peeled, Rough turned, Polished

Features:
1.Competitive price
2.Immediate delivery
3.Premium quality
4.Reliable service
5.MOQ: 1 Ton

Packing details In seaworthy packing, as your requirement.
Delivery details within 30-50 days

Chemical Composition(%)

Steel Grade C Si Mn P S Cr Mo
440C 0.95-1.20 1.0 max 1.0 max 0.040 max 0.030 max 16.0-18.0 0.75 max
1.4125 0.95-1.20 1.0 max 1.0 max 0.040 max 0.030 max 16.00-18.00 0.40-0.60



Mechanical Properties
Hardness(HB):
285max


Heat Treatment and Fabrication

Hot Working: 440C stainless steel is pre-heated at 760°C (1400°F). Temperature can be increased up to 1038-1204°C (1900-2200°F). It should not be heated below 927°C (1700°F). It is then slowly cooled at room temperature and fully annealed.
Cold Working: 440C stainless steel is slightly cold workable using common practices.
Forging: 440C stainless steel can be forged by heating slowly and uniformly to 1050-1150°C, allowing sufficient time for the steel to become heated through. Ensure not to overheat as this can cause a loss of toughness and ductility. Do not forge below 900°C reheating if necessary. After forging cool slowly in furnace or thermoinsulating material, then anneal immediately. Air cooling after forging may cause cracking.
Annealing: 440C stainless steel is annealed at 843-871°C (1550-1600°F) followed by slowly cooling in the furnace.
Hardening: 440C stainless steel can be hardened by heating at 760°C (1400°F). Temperature can be increased up to 1010°C (1850°F) followed by cooling in air or oil.
Tempering: 440C stainless steel can be tempered by soaking at 148°C (300°F).
Welding: 440C stainless steel is not welded because it can be easily air hardened. To weld this alloy, it should be preheated to 260°C (500°F) and post weld treated at 732-760°C (1350-1400°F) for 6 h followed by slowly cooling in the furnace to prevent cracking.
Machinability: 440C stainless steel can be machined in the annealed condition. Chip breakers can be used to handle tough and stringy chips. Carbide or ceramic tooling is preferred for this alloy.


Applications:
Suitable for applications requiring a combination of excellent wear resistance with moderate corrosion resistance, 440C stainless steel is commonly used in the oil and gas, marine, food and medical industries. Typical applications are pumps, valve components, bearings, knives, surgical tools, cutlery, bearings and races.


Introduction:
440C stainless steel is a high carbon martensitic stainless steel. It has high strength, moderate corrosion resistance, and good hardness and wear resistance.

Hot Tags: 440c stainless steel 1.4125 uns s44004, China 440c stainless steel 1.4125 uns s44004 suppliers, SS409 Stainless Steel Welded Pipe, SS410 Stainless Steel Plate, Corrugated SS Roof Sheet, 400 2 4360 Alloy Pipe, Stainless Steel 316 316L 316Ti Sheets And Plates, ASTM A240 Grade 431 10mm Stainless Steel Plate