42CrMo AISI 4140 Steel Specification Φ16x2500mm Cold Drawn Alloy Steel 42CrMo4 Normalized Quenched
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 42crmo aisi 4140 steel specification φ16x2500mm cold drawn alloy steel 42crmo4 normalized quenched in China. If you're going to wholesale high quality 42crmo aisi 4140 steel specification φ16x2500mm cold drawn alloy steel 42crmo4 normalized quenched made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
42CrMo AISI 4140 Steel Specification Φ16x2500mm Cold Drawn Alloy Steel 42CrMo4 Normalized Quenched
Description
| Steel Grade: | Alloy Steel | Alloy Or Not: | Is Alloy |
|---|---|---|---|
| Technique: | Hot Rolled,Cold Drawn | Type: | Alloy Steel Bar |
| Standard: | ASTM,DIN | Shape: | Round |
| Product Name: | 42CrMo4 Qt Alloy Steel Round Bars | Heat Treatment: | Normalized +Annealed +Quenched + Tempered |
| High Light: |
42CrMo alloy steel bar,AISI 4140 alloy steel bar,16 mm alloy steel bar |
||
42CrMo Steel Specification Φ16x2500mm Cold Drawn Alloy Steel 42CrMo4 Normalized Quenched
1: AISI 4140 steel introduction
AISI 4140 is defined as a low alloy steel which has 1% Cr-Mo as strengthening alloy elements.Compared with AISI 4130, it has a higher carbon content with good balance of strength, toughness ,abrasion and impact resistance and heat treatment capabilities,but poor in weldability characteristics.AISI 4140 is generally supplied in quenched and tempered condition with hardness 28-32HRC
2: AISI 4140 Steel equivalent
| Country | China | Japan | Germany | USA | British |
| Standard | GB/T 3077 | JIS G4105 | DIN (W-Nr.) EN 10250 |
AISI/ASTM ASTM A29 |
BS 970 |
| Grade | 42CrMo | SCM440 | 42crmo4/1.7225 | 4140 | EN19/709M40 |
3: AISI 4140 steel chemical composition
| Grade | C | Si | Mn | P | S | Cr | Mo | Ni |
| 42CrMo | 0.38-0.45 | 0.17-0.37 | 0.5-0.80 | ≤0.035 | ≤0.035 | 0.9-1.2 | 0.15-0.25 | - |
| SCM440 | 0.38-0.43 | 0.15-0.35 | 0.6-0.85 | ≤0.035 | ≤0.04 | 0.9-1.2 | 0.15-0.30 | - |
| 42crmo4/1.7225 | 0.38-0.45 | ≤ 0.4 | 0.6-0.9 | ≤0.025 | ≤0.035 | 0.9-1.2 | 0.15-0.30 | - |
| 4140 | 0.38-0.43 | 0.15-0.35 | 0.75-1.00 | ≤0.035 | ≤0.04 | 0.8-1.1 | 0.15-0.25 | - |
| EN19/709M40 | 0.35-0.45 | 0.15-0.35 | 0.5-0.80 | ≤0.035 | ≤0.035 | 0.9-1.5 | 0.2-0.40 | - |
4: AISI 4140 steel mechanical properties(for guidance only)
| Grade | Tensile strength σb(MPa) |
Yield strength σs (MPa) |
Elongation δ5 (%) |
Reduction ψ (%) |
Impact Value Akv (J) |
Hardness |
| 4140 | ≥1080 | ≥930 | ≥12 | ≥45 | ≥63 | 28-32HRC |
5: AISI 4140 steel overviews
| Size | Round | Dia 6-1200mm |
| Plate/Flat/Block | Thickness 6mm-500mm |
|
| Width 20mm-1000mm |
||
| Heat treatment | Normalized ; Annealed ; Quenched ; Tempered | |
| Surface condition | Black; Peeled; Polished; Machined; Grinded; Turned; Milled | |
| Delivery condition | Forged; Hot rolled; Cold drawn | |
| Test | Tensile strength, Yield strength, elongation, area of reduction, impact value, hardness, grain size, ultrasonic test, US inspection, magnetic particle testing, etc. | |
| Payment terms | T/T;L/C;/Money gram/ Paypal | |
| Trade terms | FOB; CIF; C&F; etc.. | |
| Delivery time | 30-45 days | |
| Application | AISI 4140 steel finds many applications as forgings for the aerospace,oil and gas,automotive, agricultural and defense industries etc. Typical applications for 4140 steel uses include:forged gears,spindles,fixtures,jigs,collars,Axles,conveyor parts,crow bars,logging parts,shafts,sprockets,studs,pinions,pump shafts, rams, and ring gears etc |
|
6: Delivery condition
For hot forged or hot rolled bar, usually the delivery condition is hot forged or rolled, annealed, rough turned.
For hot forged plate, usually the delivery condition is hot forged, annealed, milled surface.
For hot rolled plate, usually the delivery condition is hot rolled, annealed, black surface.



Hot Tags: 42crmo aisi 4140 steel specification φ16x2500mm cold drawn alloy steel 42crmo4 normalized quenched, China 42crmo aisi 4140 steel specification φ16x2500mm cold drawn alloy steel 42crmo4 normalized quenched suppliers, SS431 Stainless Steel Plate, 400 2 4360 Alloy Pipe, Corrugated SS Roof Sheet, 1 4510 Stainless Steel Patterned Plate, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, Stainless Steel 316 316L 316Ti Sheets And Plates