410S Stainless Steel Plate
video

410S Stainless Steel Plate

410S Stainless Steel is a non-hardening modification of Type 410. Control of the chemistry balance (low carbon and optional additions of Ti or Nb) minimizes austenite formation at high temperatures, restricting the alloy's ability to harden.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 410s stainless steel plate in China. If you're going to wholesale high quality 410s stainless steel plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

410S Stainless Steel is a non-hardening modification of Type 410. Control of the chemistry balance (low carbon and optional additions of Ti or Nb) minimizes austenite formation at high temperatures, restricting the alloy's ability to harden. The material remains soft and ductile even when the material is rapidly cooled from above the critical temperature. This low hardening characteristic helps to prevent cracking when the steel is welded or exposed to high temperatures. The alloy is ferritic in the annealed condition and ferromagnetic.

 

Because 410S cools from elevated temperatures without hardening, it is particularly useful for annealing boxes, quenching racks, oxidation resistant partitions and other high-temperature units. It also is used in the petrochemical industry for tower packing and distillation trays.

01

Element Type 410S
Carbon 0.08 max.
Manganese 1.00 max.
Sulfur 0.030 max.
Phosphorus 0.040 max.
Silicon 1.00 max.
Chromium 11.5 – 13.5
Nickel 0.60 max.
Type Yield Strength 0.2% offset (KSI) Tensile Strength (KSI) % Elongation (2″ Gauge length)
410S 30 min. 60 min. 22 min.

Hot Tags: 410s stainless steel plate, China 410s stainless steel plate suppliers, SS431 Stainless Steel Plate, SS409 Stainless Steel Welded Pipe, Stainless Steel 316 316L 316Ti Sheets And Plates, Corrugated SS Roof Sheet, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, 1 4510 Stainless Steel Patterned Plate