Alloy 321 (UNS S32100) is a titanium stabilized austenitic stainless steel with good general corrosion resistance. It has excellent resistance to intergranular corrosion after exposure to temperatures in the chromium carbide precipitation range of 800 – 1500°F (427 – 816°C). The alloy resists oxidation to 1500°F (816°C) and has higher creep and stress rupture properties than alloys 304 and 304L. It also possesses good low temperature toughness.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 321/321h stainless steel plate and sheet in China. If you're going to wholesale high quality 321/321h stainless steel plate and sheet made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

321/321H STAINLESS STEEL Plate

Product Details

Alloy 321 (UNS S32100) is a titanium stabilized austenitic stainless steel with good general corrosion resistance. It has excellent resistance to intergranular corrosion after exposure to temperatures in the chromium carbide precipitation range of 800 – 1500°F (427 – 816°C). The alloy resists oxidation to 1500°F (816°C) and has higher creep and stress rupture properties than alloys 304 and 304L. It also possesses good low temperature toughness.

 

Alloy 321H (UNS S 32109) is the higher carbon (0.04 – 0.10) version of the alloy. It was developed for enhanced creep resistance and for higher strength at temperatures above 1000oF (537°C). In most instances, the carbon content of the plate enables dual certification.

 

Alloy 321 cannot be hardened by heat treatment, only by cold working. It can be easily welded and processed by standard shop fabrication practices.

 

Typical Analysis

321 Cr% Ni% Mo% Ti% C% Cu% Mn% Si% N%
MIN 17.0 9.0 - (5xC+N) - - - 0.25 -
MAX 19.0 12.0 0.75 0.7 0.08 0.75 2.0 1.0

0.1

Hot Tags: 321/321h stainless steel plate and sheet, China 321/321h stainless steel plate and sheet suppliers, ASTM A240 Grade 431 10mm Stainless Steel Plate, SS410 Stainless Steel Plate, SS431 Stainless Steel Plate, 1 4510 Stainless Steel Patterned Plate, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, SS409 Stainless Steel Welded Pipe