Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 316l stainless steel plate in China. If you're going to wholesale high quality 316l stainless steel plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Stainless steel SS 316L is an austenitic grade stainless steel. SS 316L contains an addition of molybdenum that gives it improved corrosion resistance. Stainless steel SS 316L plate is immune to grain boundary carbide precipitation (sensitization). Stainless steel SS 316L plates are ideally suited to use in heavy gauge welded components.

| FEATURES OF SS 316L PLATE | DETAILS |
|---|---|
| Standard | JIS, ASTM, AISI, GB, EN, DIN |
| Class | SS 316L |
| Dimension | 0.3mm – 100mm |
| Size (Width) | 1000mm, 1219mm, 1250mm, 1500mm, 1524mm, 2000mm |
| Size (Length) | Customizable as per requirements |
SS 316L stainless steel plate is an essential material for applications that require superior corrosion resistance, high-temperature strength, and excellent weldability. Its versatility makes it suitable for a wide range of industries, including chemical processing, marine, pharmaceutical, oil and gas, and medical. With its robust properties and long-lasting performance, SS 316L is a reliable choice for demanding environments.
Hot Tags: 316l stainless steel plate, China 316l stainless steel plate suppliers, SS409 Stainless Steel Welded Pipe, ASTM A240 Grade 431 10mm Stainless Steel Plate, SS410 Stainless Steel Plate, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, SS431 Stainless Steel Plate, 400 2 4360 Alloy Pipe