2B Stainless Steel Strip Coil 1.4113 X6CrMo17-1 AISI 434 UNS S43400 Cold Rolled Annealed
video

2B Stainless Steel Strip Coil 1.4113 X6CrMo17-1 AISI 434 UNS S43400 Cold Rolled Annealed

1.4113 X6CrMo17-1 AISI 434 UNS S43400 Cold Rolled Annealed Stainless Steel Strip Coil Ferritic Grade AISI 434 Stainless Steel Sheet Plate Strip And Coil
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 2b stainless steel strip coil 1.4113 x6crmo17-1 aisi 434 uns s43400 cold rolled annealed in China. If you're going to wholesale high quality 2b stainless steel strip coil 1.4113 x6crmo17-1 aisi 434 uns s43400 cold rolled annealed made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

1.4113 X6CrMo17-1 AISI 434 UNS S43400 Cold Rolled Annealed Stainless Steel Strip Coil

Ferritic Grade AISI 434 Stainless Steel Sheet Plate Strip And Coil

 

Stainless Steel Strip Coil Description

 

Name Stainless Steel Strip Coil
 

201,202,304,304L,309, 309S,310S,316,316L,316Ti,317L,321,347H,409,409L,

410, 410S, 420(420J1, 420J2), 430, 436, 439, 441, 444, 446 etc.

Thickness: Cold Cold : 0.3, 0.4, 0.5, 0.6, 0.7, 0.8, 0.9, 1.0, 1.2, 1.5mm
Hot Rolled: 1.6, 2.0, 2.5, 3.0, 4.0, 5.0, 6.0, 8.0, 10, 12, 14, 16 .......40 mm
Width: 1000mm,1219mm(4feet),1250mm,1500mm,1524mm(5feet),
1800mm,2000mm or as your requirements
Length: 2000mm,2440mm(8feet),2500mm,3000mm,3048mm(10feet),
5800mm, 6000mm or as your requirements
Finish:

Common: 2B, 2D, HL(Hairline), BA(Bright annealed), No.4

Colored: Gold mirror, Sapphire mirror, Rose mirror, black mirror, bronze mirror;

Gold brushed, Sapphire brushed, Rose brushed, black brushed etc.

Brand: TISCO, BAOSTEEL, POSCO, JISCO, LISCO etc.
Certification: ISO, SGS, BV, CE or as required
Application:

Architectural decoration, luxury doors, elevators decorating, metal tank shell, ship building,

decorated inside the train, as well as outdoor works, advertising nameplate, the ceiling

and cabinets, aisle panels, screen, the tunnel project, hotels, guest houses, entertainment

place, kitchen equipment, light industrial and others..

 

Molybdenum containing 17% chromium stainless steel

AISI JIS EN/DIN
434, S43400 SUS434 1.4113, X6CrMo17-1

 

434 stainless offers

good resistance to pitting corrosion

good resistance to industrial atmospheres

good resistance to salt spray corrosion

good formability

excellent polishability

 

Product ranges

 

434 stainless steel sheet, plate, strip and coil

 

 

Our Service

 

1. Immediate Respond.

All the customers have Mittel full attention, we will be 24/7 on line at your services to provide the immediate and professional suggestion. Mittel STEEL has exported to more than 30 countries in the world.
We could provide you the immediate respond services with our sincerity.

2.Professional Suggestion.

With decade commitment, more than 90% technician has incepted the mechanical bachelor degree in Lianlong team, and almost 60% has more than 6 years' steel manufacturing and consulting experiences.
We could provide you the professional suggestion with our sincerity.

3.Strict QA/QC Procedure.

as the bankable manufacturer, always cherish the quality as the lifetime.
We abide by the strict quality control(QC)ans quality Assurance(QA) procedure.

2B Stainless Steel Strip Coil 1.4113 X6CrMo17-1 AISI 434 UNS S43400 Cold Rolled Annealed 0

2B Stainless Steel Strip Coil 1.4113 X6CrMo17-1 AISI 434 UNS S43400 Cold Rolled Annealed 1

Hot Tags: 2b stainless steel strip coil 1.4113 x6crmo17-1 aisi 434 uns s43400 cold rolled annealed, China 2b stainless steel strip coil 1.4113 x6crmo17-1 aisi 434 uns s43400 cold rolled annealed suppliers, Stainless Steel 316 316L 316Ti Sheets And Plates, SS409 Stainless Steel Welded Pipe, ASTM A240 Grade 431 10mm Stainless Steel Plate, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, 1 4510 Stainless Steel Patterned Plate, SS410 Stainless Steel Plate