18 SR Stainless Steel Plate
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 18 sr stainless steel plate in China. If you're going to wholesale high quality 18 sr stainless steel plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Type 18 SR Stainless Steel provides excellent resistance to high-temperature scaling. 18SR is readily welded by conventional methods. It is not subject to embrittlement or loss of corrosion resistance in the heat-affected zones that affects many other straight chromium alloys. This alloy is especially valuable for applications requiring high-temperature scaling resistance superior to Types 409, 430 and 304 stainless steels and for those applications where Types 442 and 446 give only marginal protection.

| Element | Type 18SR |
|---|---|
| Carbon | 0.015 |
| Manganese | 0.30 |
| Chromium | 17.30 |
| Nickel | 0.25 |
| Titanium | 0.25 |
| Aluminum | 1.7 |
Industrial ovens, blowers, exhaust systems, furnace equipment, heaters, induction furnaces and furnace tubes, annealing boxes, baffle plates, heat exchangers, resistor grids, kiln liners and pyrometer tubes.
Hot Tags: 18 sr stainless steel plate, China 18 sr stainless steel plate suppliers, ASTM A240 Grade 431 10mm Stainless Steel Plate, SS409 Stainless Steel Welded Pipe, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, 400 2 4360 Alloy Pipe, Stainless Steel 316 316L 316Ti Sheets And Plates, SS410 Stainless Steel Plate