Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of sus304 astm a554 stainless steel square pipes in China. If you're going to wholesale high quality sus304 astm a554 stainless steel square pipes made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
SUS304 ASTM A554 Stainless Steel Square Pipes
| Item Name: | Stainless Steel Welded or seamless Square Tubes for Handrail | ||||||||
| Standard: | ASTM A554 or A312 | ||||||||
| Grade of Material: | AISI 201, 202, 304, 304L, 316, 316L, etc. | ||||||||
| Certificate: | ISO 9001: 2008 | ||||||||
| Dimension: | 10 mm x 10 mm - 200 mm x 200 mm (See Range Below) | ||||||||
| Wall Thickness: | 0.3 mm - 5.0 mm | ||||||||
| Surface: | Polished 320 G, 400 G, 600 G; Hairline; Descaled. | ||||||||
| Length: | 10 mm - 10000 mm | ||||||||
| Packing: | Each or several tubes (pipes) would be sleeved in plastic bag individually, and then a bundle of them would be packed by a weaving bag which is seaworthy. | ||||||||
| Application: | Decoration, construction & building, such as handrail, railing, window, furniture, etc. | ||||||||
| Chemical Composition: |
Grade of Material | C | Si | Mn | P | S | Ni | Cr | Mo |
| AISI 201 | ≤0.15 | ≤1.00 | 5.50~7.50 | ≤0.060 | ≤0.03 | 1.00 ~1.50 | 13.50~15.00 | \ | |
| AISI 202 | ≤0.15 | ≤1.00 | 7.50~10.00 | ≤0.060 | ≤0.03 | 4.00~6.00 | 17.00~19.00 | \ | |
| AISI 304 | ≤0.08 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 8.00~11.00 | 18.00~20.00 | \ | |
| AISI 304L | ≤0.035 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 8.00~13.00 | 18.00~20.00 | \ | |
| AISI 316 | ≤0.08 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 10.00~14.00 | 16.00~18.00 | 2.00~3.00 | |
| AISI 316L | ≤0.035 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 10.00~14.00 | 16.00~18.00 | 2.00~3.00 | |
| Mechanical Property: |
Grade of Material | Elongation (%) | Tensile Strengh (Rm) N/m m³ | Yield Strength (Rp) 0.2%N/m m³ | Hardness (HV) | ||||
| AISI 201 | ≥35 | ≥520 | ≥210 | ≤253 | |||||
| AISI 202 | ≥35 | ≥590 | ≥210 | ≤218 | |||||
| AISI 304 | ≥35 | ≥520 | ≥210 | ≤200 | |||||
| AISI 304L | ≥35 | ≥480 | ≥180 | ≤200 | |||||
| AISI 316 | ≥35 | ≥520 | ≥210 | ≤200 | |||||
| AISI 316L | ≥35 | ≥480 | ≥180 | ≤200 | |||||