SUS 439 Stainless Steel Pipe For Exhaust Tubing SS439M Welded 102*2
video

SUS 439 Stainless Steel Pipe For Exhaust Tubing SS439M Welded 102*2

439 stainless steel is resistant to attack by potable water and many mildly or moderately corrosive chemical environments which are oxidizing in nature. In various chloride solutions, studies have shown pitting resistance of Type 439 to be superior to that of Type 304. In addition, Type 439 is not subject to stress corrosion cracking which may cause premature failure of austenitic steels in chloride bearing environments such as hot waters used in heat exchangers.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of sus 439 stainless steel pipe for exhaust tubing ss439m welded 102*2 in China. If you're going to wholesale high quality sus 439 stainless steel pipe for exhaust tubing ss439m welded 102*2 made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

SUS 439 Stainless Steel Pipe For Exhaust Tubing SS439M Welded 102*2

Description

Steel Grade: 439 Type: Welded
Welding Line Type: ERW Standard: EN,ASTM,AISI,DIN,JIS
Application: Construction,Decoration,Industry Surface: Annealing 2D
Thickness: 0.3-3mm Length: 6 Meters Or Customized
Outer Diameter: 16-127mm Price Term: CIF,FOB,EX-WORK
High Light:

Stainless Steel Welded Pipe For Exhaust

,

SUS 439 Stainless Steel Pipe Tubing

,

Welded 102*2 Stainless Steel Pipe

SUS 439 Stainless Steel Pipe For Exhaust Tubing SS439M Stainless Steel Welded Pipe 102*2

 

439 Stainless Steel

439 stainless steel is a titanium stabilized ferritic stainless steel grade with , 18 percent chromium alloy, it designed to resist corrosion in a variety of oxidizing environments from fresh water to boiling acids, its corrosion resistance similar to that of 304/304L stainless steel. Type 439 may also be used in many oxidizing environments where Type 304 is considered adequate in terms of general corrosion resistance but is subject to chloride stress corrosion cracking. This variation does not require annealing after welding to restore ductility or to provide intergranular corrosion resistance. Type 439 also has superior formability capabilities and is heavily used in the automotive industry; it can be work hardened slightly to increase tensile strength.

Excellent resistance to stress corrosion cracking, good weldability, high thermal conductivity and low thermal expansion characteristics make Type 439 stainless steel an ideal consideration for many applications, typical applications include tubular manifolds and exhaust system components.

439 Stainless Steel Features

Stainless steel grade 439 has good weldability, brightness, and pitting corrosion resistance. It polishes well, and is good for deep drawing.

Excellent resistance to chloride stress corrosion cracking

Good general corrosion resistance, especially in fresh waters and mildly oxidizing environments

Weldability

Long term cost advantages

High thermal conductivity coefficient

Low thermal expansion coefficient

Good continuous and cyclic oxidation resistance.

Typical applications in automotive exhaust system and heat exchanger system

439 Stainless Steel Chemical Composition

Grade C Si Mn P S Cr Ni N Ti Fe
439 0.030 1.00 1.00 0.040 0.030 17.00 – 19.00 0.5 0.030 [0.20+4(C+N)]
Min, 1.10 Max;
Bal
TP439 0.07 1.00 1.00 0.040 0.030 17.00 – 19.00 0.5 0.040 [0.20+4(C+N)]
Min, 1.10 Max;
Bal

Max, %, 439 for ASTM A240 Plate, Sheet and Strip, TP439 for ASTM A268 seamless and welded tube

439 Stainless Steel Mechanical Properties

Grade Tensile Strength
(MPa) Min
Yield Strength
0.2% Proof (MPa) Min
Elongation
(% In 50mm) Min
Hardness Rockwell
B (HR B) Max
Hardness Brinell
(HB) Max
439 415 205 22 89 183
TP439 415 205 20 90 190

439 for ASTM A240 Plate, Sheet and Strip, TP439 for ASTM A268 seamless and welded tube

439 Stainless Steel Physical Properties

Physical Property Value
Density 7.70 G/Cm³
Melting Point 1505 °C
Thermal Expansion 11.0 X10^-6 /K
Modulus Of Elasticity 220 GPa
Thermal Conductivity 25.0 W/M.K
Electrical Resistivity 0.60 X10^-6 Ω .M

Equivalent Grades Of 439 Stainless Steel

USA
UNS
EU
EN
Japan
JIS
Germany
DIN
439
S43035
X3CrTi17 SUS430LX 1.4510

Corrosion Resistance:

439 stainless steel is resistant to attack by potable water and many mildly or moderately corrosive chemical environments which are oxidizing in nature. In various chloride solutions, studies have shown pitting resistance of Type 439 to be superior to that of Type 304. In addition, Type 439 is not subject to stress corrosion cracking which may cause premature failure of austenitic steels in chloride bearing environments such as hot waters used in heat exchangers.

Welding

439 stainless steel is weldable by the usual stainless steel methods including spot welding, TIG, MIG, laser and high frequency tube welding. Conventional gas shielding is used with the tungsten or metal arc process. If filler wire is added to the weld deposit, a stabilized stainless steel or a nickel base alloy should be considered in order to maintain corrosion resistance in the weld metal. For elevated temperature applications such as automotive exhaust systems, type439 and type 444 alloys would be preferred to maintain thermal expansion compatibility. Properly welded, grade 439 alloy retains the corrosion resistance and almost all of the mechanical properties of the base metal in the weld fusion and heat affected zones. Due to the titanium content, the weld metal will be free of the martensite normally associated with the ferritic stainless welds. Further, due to this titanium content, the heat affected zone is resistant to intergranular corrosive attack in environments in which the base metal is satisfactorily used. Welding this alloy even with adequate gas protection may cause some heat tint or oxidation that should be removed to insure maximum corrosion resistance.

Heat Treatment


Stainless steel 439 alloy should be annealed between 1450 and 1600°F (790 and 871°C) and quickly cooled. Cooling rates affect impact transition with slow cooling producing higher, less desirable impact transition. Ferritic stainless steels containing more than about 12% chromium have a susceptibility to a phenomenon known as 885°F (475°C) embrittlement. This embrittlement is observed as a degradation of impact properties at room temperature resulting from very long exposures in the temperature range of 700 to 1000°F (371 to 537°C). If service temperatures are cycling through this range, exposure above about 1050°F (565°C) restores the room temperature toughness properties. When there have been long dwell times near 885°F (475°C), service temperatures that cycle above about 1050°F (565°C) are beneficial rather than detrimental.

Applications

The unique blend of properties of 439 stainless steel make it a desirable choice for many applications. It has been used with 25 years of documented service in hot water tank applications requiring good overall corrosion resistance, resistance to stress corrosion cracking and good weldability. The alloy's oxidation resistance permits its use in residential furnaces and automotive exhaust system components. 439 alloy corrosion resistance, fabricability and reflective color compatibility have resulted in its use as small diameter tube to replace solid wire spokes in automotive wheelcover applications. The alloy has replaced carbon steel heat exchanger tubes without expansion joints because of its low coefficient of thermal expansion. 439 alloy higher thermal conductivity, compared to conventional stainless steel, has resulted in its choice over Type 304 in a number of feedwater heater applications. The successful application of any alloy is dependent upon many variables. It is important to consider these carefully before selecting any material, including 439 stainless steel.

Stainless steel grade 439 is capable of being made into complex shapes such as tubular manifolds and exhaust system components, where temperatures tend to go beyond the oxidation limit of grade 409 steel. 439 stainless steel is preferred where wet corrosion resistance especially to chlorides is needed.

SUS 439 Stainless Steel Pipe For Exhaust Tubing SS439M Welded 102*2 0SUS 439 Stainless Steel Pipe For Exhaust Tubing SS439M Welded 102*2 1

Hot Tags: sus 439 stainless steel pipe for exhaust tubing ss439m welded 102*2, China sus 439 stainless steel pipe for exhaust tubing ss439m welded 102*2 suppliers, 1 4509 1 4510 Pipes And Tubes, Stainless Steel High Pressure Pipe, 420J1 420J2 316 Stainless Pipe, SS410 Stainless Steel Pipe, 410 Stainless Steel Pipe, Inconel 625 Alloy Steel Plate

Send Inquiry

whatsapp

Phone

E-mail

Inquiry