Super Thin Wall Stainless Steel Tube
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of super thin wall stainless steel tube in China. If you're going to wholesale high quality super thin wall stainless steel tube made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Super thin wall stainless steel tubes are designed for applications requiring a combination of lightweight construction, high strength, and excellent corrosion resistance. These tubes are typically used in industries such as medical, aerospace, electronics, and precision instrumentation, where precision and reliability are paramount.

| Specification | Description |
|---|---|
| Outer Diameter | 0.5 mm to 50 mm |
| Wall Thickness | 0.05 mm to 1 mm |
| Length | Custom lengths available, typically up to 6 meters |
| Material | Austenitic stainless steel (e.g., 304, 316, 316L) |
| Standards | ASTM A213, ASTM A269, ASTM A270 |
| Surface Finish | Smooth, polished, or custom finishes |
| Tolerance | High precision tolerances as per industry standards |
| Weldability | Excellent weldability for various joining processes |
| Formability | Suitable for bending, flaring, and other forming processes |
| Corrosion Resistance | High, due to stainless steel composition |
Applications:
1.Fine Cylinder: Gas, air, oil, drinking water system;Cooling screw;tubes for bending machines;Compressor;highly fine processing ,etc.
2.Precise machine / instrument: Semiconductor industry (high purity gas line / instruments) ;Precise electronic / electric / automobile parts;Parts for measuring instruments;Precise shaft; Roller;Medical parts for orthodontics, etc.
3.Tubes for food/hygiene.
4.Heat exchanger: Boiler; Nuclear generator;Chemical manufacturing line;special plants,etc.
Hot Tags: super thin wall stainless steel tube, China super thin wall stainless steel tube suppliers, Stainless Steel High Pressure Pipe, Slip On Flanges, SS410 Stainless Steel Pipe, 420J1 420J2 316 Stainless Pipe, Inconel 625 Alloy Steel Plate, 410 Stainless Steel Pipe