SS904L Stainelss Steel Seamless Pipe
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of ss904l stainelss steel seamless pipe in China. If you're going to wholesale high quality ss904l stainelss steel seamless pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
SS 904 L seamless pipe, as the name suggests, is a pipe without a seam or a weld-joint made in stainless steel 904L grade. SS 904 L seamless pipe is made from a solid round steel 'billet'. The billet is heated and pushed or pulled over a form until the steel is shaped into a hollow pipe.
SS 904 L seamless pipe is made of 904L grade which is a low carbon high alloy austenitic stainless steel.
SS 904 L seamless pipe has a high resistance to pitting in chloride solutions, a high resistance to both crevice and stress corrosion cracking. SS 904 L seamless pipes are far better than other austenitic stainless steels due to the higher percentage of nickel and molybdenum.

| Grade | 904L |
| Tensile Strength (MPa) min | 490 |
| Yield Strength 0.2% Proof (MPa) min | 220 |
| Elongation (% in 50mm) min | 35 |
| Hardness | |
| Rockwell B (HR B) max | 70-90 typical |
| Brinell (HB) max | - |
Hot Tags: ss904l stainelss steel seamless pipe, China ss904l stainelss steel seamless pipe suppliers, SS410 Stainless Steel Pipe, 420J1 420J2 316 Stainless Pipe, Inconel 625 Alloy Steel Plate, 1 4509 1 4510 Pipes And Tubes, Slip On Flanges, Stainless Steel High Pressure Pipe