SS904 904L Stainless Steel Pipes
video

SS904 904L Stainless Steel Pipes

Pipes have good resistance to hot corrosion in multiple environments. These 904L pipes are high-alloy austenitic stainless steel with low carbon content. It contains carbon, chromium, copper, manganese, molybdenum, nickel, phosphorous, sulphur, silicon. It shows good resistance to pitting and crevice corrosion. Also, it shows some properties like good resistance to stress corrosion cracking, intergranular corrosion & good formability, and also weldability.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of ss904 904l stainless steel pipes in China. If you're going to wholesale high quality ss904 904l stainless steel pipes made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Pipes have good resistance to hot corrosion in multiple environments. These 904L pipes are high-alloy austenitic stainless steel with low carbon content. It contains carbon, chromium, copper, manganese, molybdenum, nickel, phosphorous, sulphur, silicon. It shows good resistance to pitting and crevice corrosion. Also, it shows some properties like good resistance to stress corrosion cracking, intergranular corrosion & good formability, and also weldability.

219 115

These grade is usually intended for use under severe corrosive conditions. It has an application which is proved over many years, and it was originally developed to resist corrosion in dilute sulfuric acid. These pipes are standardized and approved for pressure vessel use in several countries. The structural pipe is fully austenitic stainless steel and is less sensitive to precipitation ferrite and sigma phases than the other conventional austenitic grades with high molybdenum content. Because of the relatively high contents of chromium, nickel, molybdenum, and copper have good resistance to general corrosion, particularly in sulfuric and phosphoric conditions.

Grade UNS DIN JIS EN BS AFNOR
SS 904L N08904 1.4539 SUS 904L X1NiCrMoCu25-20-5 904S13 Z2 NCDU 25-20
Grade C Mn Si P S Cr Mo Ni Cu
SS 904L 0.020 max 2.00 max 1.00 max 0.040 max 0.030 max 19.00 – 23.00 4.00 – 5.00 max 23.00 – 28.00 1.00 – 2.00

219 219

 

Mechanical Properties of Stainless Steel 904L Pipe
Density: 7.95 g/cm3
Melting Point: 1350 °C (2460 °F)
Tensile Strength: Psi – 71000, MPa – 490
Yield Strength (0.2% Offset): Psi – 32000, MPa – 220
Elongation: 35 %

These Stainless Steel 904L Pipes are used in Shore oil drilling companies, power generation, petrochemicals, gas processing, speciality chemicals. Also, it is used in the pharmaceutical industry, chemical equipment, seawater equipment, heat exchangers, condensers, and pulp and paper industry. The significant inclusion of nickel elements to the alloy of stainless steel 904L makes it possible for the pipes to have an outstanding performance even in elevated settings.

 

Along with it is a non-magnetic alloy, the Stainless Steel 904L Pipe also exhibits good resistance to stress-related corrosion cracking. Because of the presence of molybdenum element in the alloy is reduces the occurrence of crevice corrosion. Along with this, it is used in applications between moderate to high temperatures.

Hot Tags: ss904 904l stainless steel pipes, China ss904 904l stainless steel pipes suppliers, Slip On Flanges, Inconel 625 Alloy Steel Plate, 420J1 420J2 316 Stainless Pipe, Stainless Steel High Pressure Pipe, 1 4509 1 4510 Pipes And Tubes, SS410 Stainless Steel Pipe