SS 420 is made of 420-grade stainless steel, a higher carbon version of stainless steel which can be heat-treated. The tube SS420 contains at least 12% chromium, enough to give tube SS 420 resistance to corrosion.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of ss420 stainless steel tube in China. If you're going to wholesale high quality ss420 stainless steel tube made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

SS 420 is made of 420-grade stainless steel, a higher carbon version of stainless steel which can be heat-treated. The tube SS420 contains at least 12% chromium, enough to give tube SS 420 resistance to corrosion.

The 420 tube of infinite steel is a straight chromium steel that is not hardenable and is a ferritic group of steels. Stylish steel 420 tube, combined with practical mechanical properties, is known for its good corrosion, formability and formability. Stainless steel 420 tubes improve their corrosion resistance by their molybdenum content.

219 195


SS 420 tubes also have extraordinary resistance to stress corrosion cracking.

Element C Mn Si P S Cr
420 0.15 max 1.00 max 1.00 max 0.04 max 0.03 max

min: 12.0

max: 14.0