Series ASTM AISI SUS 201 304 316 430
video

Series ASTM AISI SUS 201 304 316 430

0.3-60mm Seamless Stainless Steel Pipe/Tube 200 300 400 Series ASTM AISI SUS 201 304 316 430
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of series astm aisi sus 201 304 316 430 in China. If you're going to wholesale high quality series astm aisi sus 201 304 316 430 made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Series ASTM AISI SUS 201 304 316 430

Product Details

0.3-60mm Seamless Stainless Steel Pipe/Tube 200 300 400 Series ASTM AISI SUS 201 304 316 430

DELIVERY DETAILS

1. We will count cheapest shipping cost and send it to your email.
2. Start production immediately after receiving the advance payment.
3. About 10-15 working days to complete the production, and then the customer side to pay the balance.

All the products you purchase will be strictly packaged to ensure the integrity of the goods in shipment.All the goods will be made, loaded, transported, put in containers, ship, sea transportation, etc. We will try to ensure your arrival time and the goods are delivered on time over time.

Product Description

Size Outer Diameter Seamless: 6-500mm or Customized
Wall Thickness 0.5-150mm or Customized
Length 1-12m as customer requirement
Material 201,304,309S,310S,316,316L,316Ti,317,317L,321,904L,430, etc
Surface Fnished No.1 No.3 No.4 HL 2B BA 4K 8K 1D 2D
Testing Methods Pressure test,Flaw detection,Eddy current testing, Hydrostatic testing or Ultrasonicexamination and also with chemical and physical property inspection
Standard

ASTM A213,A312,ASTM A269,ASTM A778,ASTM A789,DIN 17456, DIN17457,DIN 17459,JIS G3459,JISG3463,GOST9941,EN10216, BS3605,GB13296

Application Food processing equipment, particularly in beer brewing, milk processing & winemaking
Kitchen benches, sinks, troughs, equipment and appliances
Architectural paneling, railings & trim
Chemical containers, including for transport
Heat Exchangers
Woven or welded screens for mining, quarrying & water filtration
Pipe fittings.
Container Size 20ft GP:5898mm(Length)x2352mm(Width)x2393mm(High) 24-26CBM

40ft GP:12032mm(Length)x2352mm(Width)x2393mm(High) 54CBM

40ft HC:12032mm(Length)x2352mm(Width)x2698mm(High) 68CBM

H30d615519ed54348a61d28849d73728aAjpg100x100xz

Hot Tags: series astm aisi sus 201 304 316 430, China series astm aisi sus 201 304 316 430 suppliers, 1 4509 1 4510 Pipes And Tubes, 410 Stainless Steel Pipe, SS410 Stainless Steel Pipe, Inconel 625 Alloy Steel Plate, 420J1 420J2 316 Stainless Pipe, Stainless Steel High Pressure Pipe

Send Inquiry

whatsapp

Phone

E-mail

Inquiry