Seamless 304/304L Stainless Steel Tubing | SAE J3129
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of seamless 304/304l stainless steel tubing | sae j3129 in China. If you're going to wholesale high quality seamless 304/304l stainless steel tubing | sae j3129 made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
The seamless tubing shall be made from stainless steel conforming to the chemical composition of S30400 or S30403 as specified in ASTM A269. The SAE J3129 seamless SS304/304L tubing shall be cold drawn and annealed to produce a finished product and shall meet all requirements of ASTM A269. After production is finished, tubes shall be bright annealed and passivated. Oxide annealed, pickled, and passivated can be supplied by agreement between producer and purchaser. Centerless grinding is not permitted; however, a light polish to improve surface appearance is permitted. Polished tubing must be subsequently passivated.

The seamless ss 304/304L tubing manufactured in accordance with SAE J3129 shall satisfactorily meet the following performance tests according to ASTM A1016: flattening test, flaring test, reverse flattening test, tensile test, elongation test, pressure proof test, eddy current test, and ultrasonic test.
The tubes shall be straightened to a tolerance of 1 mm over a 1000 mm length. Finished tubes shall have smooth end free of burrs. The surface condition of the tube is critical in order to prevent possible leak paths on double flare fittings, mechanical form fittings, or other applications where the outside or inside surface of the tube becomes the sealing surface. The surface of the tube shall be free of excessive roll marks, score marks, chatter marks, or the other surface imperfections that are considered detrimental to the function of the tubing. The tubing may be packaged in straight lengths or coils, in sea-worthy firm plywood cases.
Hot Tags: seamless 304/304l stainless steel tubing | sae j3129, China seamless 304/304l stainless steel tubing | sae j3129 suppliers, Inconel 625 Alloy Steel Plate, 410 Stainless Steel Pipe, 420J1 420J2 316 Stainless Pipe, SS410 Stainless Steel Pipe, Slip On Flanges, 1 4509 1 4510 Pipes And Tubes