Length 6000mm Seamless Stainless Steel Pipe SS316L / TP316L Astm A312 OD 89mm X Thk 4mm
video

Length 6000mm Seamless Stainless Steel Pipe SS316L / TP316L Astm A312 OD 89mm X Thk 4mm

Length 6000mm Seamless Stainless Steel Pipe SS316L / TP316L Astm A312 OD 89mm X Thk 4mm Description Application: Construction Standard: DIN,ASTM,JIS,AISI Steel Grade: 300 Series,304 304L 316 316L 310S 321 Type: Seamless Welding Line Type: Seamless Thickness: 1mm-20mm Length: 3000mm~6000mm Shape: Round.square.Rectangle Outer Diameter: 6-630mm Technique: Cold Drawn Surface: Annealing,pickling,polishing Color: Customerized High Light: 4mm Seamless Stainless Steel Pipe , TP316L Seamless Stainless Steel Pipe , SS316L Stainless Steel Seamless Tube
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of length 6000mm seamless stainless steel pipe ss316l / tp316l astm a312 od 89mm x thk 4mm in China. If you're going to wholesale high quality length 6000mm seamless stainless steel pipe ss316l / tp316l astm a312 od 89mm x thk 4mm made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Length 6000mm Seamless Stainless Steel Pipe SS316L / TP316L Astm A312 OD 89mm X Thk 4mm

Description

Application: Construction Standard: DIN,ASTM,JIS,AISI
Steel Grade: 300 Series,304 304L 316 316L 310S 321 Type: Seamless
Welding Line Type: Seamless Thickness: 1mm-20mm
Length: 3000mm~6000mm Shape: Round.square.Rectangle
Outer Diameter: 6-630mm Technique: Cold Drawn
Surface: Annealing,pickling,polishing Color: Customerized
High Light:

4mm Seamless Stainless Steel Pipe

,

TP316L Seamless Stainless Steel Pipe

,

SS316L Stainless Steel Seamless Tube

Length 6000mm SS316L / TP316L Stainless Steel Seamless Tube Astm A312 OD 89mm X Thk 4mm

Product Description

Mittel located in Jiangsu province,China.

Produce and stock 300 series and duplex stainless steel pipe,fitting and flange.

Production range for stainless steel fitting:
OD:6mm-1600mm
Grade:304,304L,316,316L,321,347H,904L,duplex and super suplex.

We also keep 500tons stock, stock item can be delivered in 7days.

Material Stainless Steel Seamless Pipe
Steel Grade 200 Series: 201,202
300 Series: 301,304,304L,304H,316,316L,316Ti,317L,321,309s,310s
400 Series: 403,405,409L,410,416,420,431, 434
Duplex Steel: 904L,2205,2507,2101,2520,2304
Thickness 0.1mm-100mm (as required)
Length 6m,9m,12m (as required)
Surface Pickling,Polished,Bright,Hairline
Technique Cold Rolled, Hot Rolled
Treatment Welded or Seamless
Welding Line Type ERW,EFW,Seamless,Spiral Welded
Shape Round,Square,Rectangular,Oval
Color Golden/Rose Gold/Silver/Black/Red/Green/Blue/as required
Tolerance As standard
Delivery Time 7-10days
Payment Terms T/T, L/C, D/P, Paypal, Trade Online
MOQ 0.5 Ton
Application Liquid transport, Boiler pipe, Hydraulic,Automobile,Mining, Construstion

 

 

Nominal Outside Diameter Sch 5S Sch 10S Sch-40S Sch-80S Sch-160S Sch-XXS
mm inch mm WT mm Weight (Kg/mt) WT mm Weight (Kg/mt) WT mm Weight (Kg/mt) WT mm Weight (Kg/mt) WT mm Weight (Kg/mt) WT mm Weight (Kg/mt)
3 1/8 10.3 1.24 0.276 1.24 0.28 1.73 0.37 2.41 0.47 - - - -
6 1/4 13.7 1.24 0.390 1.65 0.49 2.24 0.631 3.02 0.80 - - - -
10 3/8 17.1 1.24 0.490 1.65 0.63 2.31 0.845 3.20 1.10 - - - -
15 1/2 21.3 1.65 0.800 2.11 1.00 2.77 1.27 3.75 1.62 4.75 1.94 7.47 2.55
20 3/4 26.7 1.65 1.03 2.11 1.28 2.87 1.68 3.91 2.20 5.54 2.89 7.82 3.63
25 1 33.4 1.65 1.30 2.77 2.09 3.38 2.50 4.55 3.24 6.35 4.24 9.09 5.45
32 1 1/4 42.2 1.65 1.65 2.77 2.70 3.56 3.38 4.85 4.47 6.35 5.61 9.70 7.77
40 1 1/2 48.3 1.65 1.91 2.77 3.11 3.68 4.05 5.08 5.41 7.14 7.25 10.16 9.54
50 2 60.3 1.65 2.40 2.77 3.93 3.91 5.44 5.54 7.48 8.74 11.1 11.07 13.44
65 2 1/2 73.0 2.11 3.69 3.05 5.26 5.16 8.63 7.01 11.4 9.53 14.9 14.2 20.39
80 3 88.9 2.11 4.51 3.05 6.45 5.49 11.30 7.62 15.2 11.1 21.3 15.24 27.65
100 4 114.3 2.11 5.84 3.05 8.36 6.02 16.07 8.56 22.3 13.49 33.54 17.12 41.03
125 5 141.3 2.77 9.47 3.40 11.57 6.55 21.8 9.53 31.97 15.88 49.11 19.05 57.43
150 6 168.3 2.77 11.32 3.40 13.84 7.11 28.3 10.97 42.7 18.2 67.56 21.95 79.22
200 8 219.1 2.77 14.79 3.76 19.96 8.18 42.6 12.7 64.6 23.0 111.2 22.23 107.8
250 10 273.1 3.40 22.63 4.19 27.78 9.27 60.5 12.7 96.0 28.6 172.4 25.40 155.15
300 12 323.9 3.96 31.25 4.57 36.00 9.52 73.88 12.7 132.0 33.32 238.76 25.40 186.97
350 14 355.6 3.96 34.36 4.78 41.3 11.13 94.59 19.05 158.08 35.71 281.70 - -
400 16 406.4 4.19 41.56 4.78 47.29 12.7 123.30 21.41 203.33 40.46 365.11 - -
450 18 457.2 4.19 46.80 4.78 53.42 14.27 155.80 23.8 254.36 45.71 466.40 - -
500 20 508.0 4.78 59.25 5.54 68.71 15.09 183.42 26.19 311.2 49.99 564.68 - -
600 24 609.6 5.54 82.47 6.35 94.45 17.48 255.41 30.96 442.08 59.54 808.22 - -


Stainless Steel Seamless Pipe Tp316L A213 Heat Exchanger Tube Facotry
Mittel has always inculcated and followed sten quality standards for all of its manufacturing processes.

All the materials used are of premium quality and compatible with latest machineries and manufacturing

technologies. The technical and commercial quality guidelines of PMC are set to high standards.

A quality control team supervises quality assurance and control aspects along with the entire process

system by recognizing and associating with the quality circle. The quality control tests are conducted

regularly in order to maintain a consistent and uniform product quality.

  Destructive Testing        
           
• Tensile Test • Flaring Test • IGC Test - Prac A,B,C&E
• Hardness Test • Flange Test • Reverse Flattening Test
• Flattening Test • Reverse Test - Bend Test • Impact Test
           
           
  Non- Destructive Testing        
           
• Hydrostatic Test • P.M.I Test • Dye Penetrant Test
• Eddy Current Test • Spectro Test • Baroscopic Test
• Air Under Water Test • Ultrasonic Test    


VALUE-ADD SERVICES BY MITTEL

Stainless steel pipe polish Stainless can polish nearly any stainless steel pipe item to a #4 polish, #6 Polish, #7 polish or a #8 mirror finish. Stainless steel polished pipes can also be cut to size.
Stainless Steel Pipe Beveling Stainless can bevel the edges of stainless steel plate to prepare for welding or other processes.
Stainless Steel Pipe Honing & Turning Stainless can hone pipe and tube, using a precision abrasion process in order to obtain a desired finish or close dimensional tolerance.
Heatreating & Annealed Some grades of stainless steel pipe can be heatreated to change the mechanical properties.
Positive Material Identification (PMI) Stainless can perform PMI testing in house for most stainless steel grades, or we can work with independent labs to complete PMI in order to meet customer specifications.
UT Testing In some cases, UT testing of the stainless steel plates may be required. We can assist you with this requirement.

 

 

Packaging & Shipping

Stainless Steel ASTM A312/A213/A269 Tp316L/TP304/TP304L Cold/Hot Rolled Seamless Steel Pipe/Tube
Stainless Steel ASTM A312/A213/A269 Tp316L/TP304/TP304L Cold/Hot Rolled Seamless Steel Pipe/Tube

Shipping:

 

1. WORLDWIDE SHIPPING. (Except some countries and APO/FPO)

2. Goods delivered by 20" , 40" FCL/LCL by quantity or customer's request.

3. Customers specifying freight forwarders or negotiable shipping methods!

4. Delivery Time: 10-30days after conformed or according to quantity.



 

About Us

MITTEL .is one of the leading manufacturer and exporter for the Stainless Steel Seamless Pipes & Tubes from Wuxi, China. Based on our Stainless Steel seamless pipe factory, We supply the ONE-STOP service fittings,flanges, valves etc to our customers home and abroad.

 

We manufacture strictly as per the standard, We have mechanical properties test machine, supersonic testing machine, eddying current test machine, hydrostatic test machine, and spectrum analyzer for chemical composition.etc equipment to insure manufacturing processes and inspection and final quality guarantee.


We welcome customers themselves and/or their appointed third party inspection such as SGS,BV,MOODY, LIoyd's,TUV,DNV Etc well-known third party to conduct the inspection to our company and our products.

 

FAQ

Q What is our product range?
A Based on our Stainless Steel seamless pipe factory, We supply the ONE-STOP service fittings,flanges, valves etc
Q What is our advantages?
A

1.MITTEL has more than 10 years experience in this industry.

2.For each order, strict QC will be carried by the QC department before Shipping

3.Certificated by ISO,PED,TUV

4.Third party inspection such as TUV,BVmLloyd's,SGS.

5.Competitive price with reliable quality

 

Length 6000mm Seamless Stainless Steel Pipe SS316L / TP316L Astm A312 OD 89mm X Thk 4mm 3

 

Length 6000mm Seamless Stainless Steel Pipe SS316L / TP316L Astm A312 OD 89mm X Thk 4mm 4Length 6000mm Seamless Stainless Steel Pipe SS316L / TP316L Astm A312 OD 89mm X Thk 4mm 5

Hot Tags: length 6000mm seamless stainless steel pipe ss316l / tp316l astm a312 od 89mm x thk 4mm, China length 6000mm seamless stainless steel pipe ss316l / tp316l astm a312 od 89mm x thk 4mm suppliers, Inconel 625 Alloy Steel Plate, 1 4509 1 4510 Pipes And Tubes, Stainless Steel High Pressure Pipe, Slip On Flanges, 420J1 420J2 316 Stainless Pipe, 410 Stainless Steel Pipe

Send Inquiry

whatsapp