JIS G3459 SUS304 Stainless Steel Seamless Pipe
Manufacture:welded process,
Outside Diameter:12.7mm——127mm
Wall thickness:0.9mm——12.7mm
Length:6000mm、12000m or specified length as require
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of jis g3459 sus304 stainless steel seamless pipe in China. If you're going to wholesale high quality jis g3459 sus304 stainless steel seamless pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
JIS G3459 SUS304 stainless steel seamless pipe is a stainless steel seamless pipe that complies with the Japanese Industrial Standard (JIS G3459), and the main material is SUS304 stainless steel.
SUS304 stainless steel pipe is a commonly used stainless steel material with good corrosion resistance and can remain stable in a variety of environments. It is easy to process and form, and is suitable for production processes such as cold drawing.
SUS304 seamless pipes are widely used in various fields, including automobiles, solar energy, home appliances, precision electronics, pressure vessels, nuclear power, chemical equipment, etc.
Products Data
Heat treatment of JIS G3459 SUS304 Stainless Steel Pipe
| Classification | Grade | Solution treatment ℃ |
| Austenitic pipes | SUS 304TP | 1010 min, rapid cooling |
Chemical composition of SUS304 Stainless Steel Thick Wall Pipe
| Grades | Chemical composition | ||||||
| C | Si | Mn | P | S | Ni | Cr | |
| SUS 304 TP | 0.08 max. | 1.00 max. | 2.00max. | 0.040 max. | 0.030 max. | 8.00~11.00 | 18.00~20.00 |
Mechanical properties of SUS304 Stainless steel round tube
|
Grade |
Mechanical properties | |||||
| Tensile strength | Yield Strength | Elongation % | ||||
| kgf/mm 2 {N/mm2} | kgf/mm 2 {N/mm2} |
No. 11 test piece No. 12 test piece |
No.5 test piece | No.4 test piece | ||
| Longitudinal direction | Transverse direction | Longitudinal direction | Transverse direction | |||
| SUS 304 TP | 53{520}min. | 21{206} min | 35 min | 25 min | 30 min | 22 min |
Products Display
JIS G3459 SUS304 Stainless steel heat exchanger tubes

Why choosing GNEE
GNEE conventional diameters of 19mm, 25mm, 32mm, and 38mm are in stock and can be made to length as required, with the longest length being 30m. Depending on the application, two processes can be used: cold drawing (annealing and pickling for soft industrial tubes) and cold rolling (uniform wall thickness, hard without annealing, bright inside and outside, and soft industrial tubes after annealing).
If you have any inquiry, please don't hesitate to contact us immediately! Free Quote ss@gneesteel.com
GNEE CUSTOMER VISIT

GNEE FACTORY ENVIRONMENT

GNEE PACKAGING AND SHIPPING

FAQ
Q: Do you have any certifications?
A: Yes,that's what we guarantee to our clients. we have IS09000,IS09001 certinicate,APISL PSL-1 CE certificates etc.Our products are of high quality and we have professional engineers and development team.
Q: Do you accept the third party inspection?
A: Yes absolutely we accept.
Q:Will you delivery the goods on time?
A: Yes,we promise to provide best quality products and delivery on time no matter if the price change lot or not. Honesty is our company's tenet.
Hot Tags: jis g3459 sus304 stainless steel seamless pipe, China jis g3459 sus304 stainless steel seamless pipe suppliers, SS410 Stainless Steel Pipe, Stainless Steel High Pressure Pipe, 1 4509 1 4510 Pipes And Tubes, Inconel 625 Alloy Steel Plate, 410 Stainless Steel Pipe, Slip On Flanges