ASTM554 TP304 Stainless Steel Square Pipe Welding
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of astm554 tp304 stainless steel square pipe welding in China. If you're going to wholesale high quality astm554 tp304 stainless steel square pipe welding made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
ASTM554 TP304 Stainless Steel Square Pipe Welding
Product Description
ASTM554 TP304 Stainless Steel Square Pipe Welding
Product Introduction
Stainless steel square pipe is one type of the stainless steel special shaped tube.
generally used for structural purposes and applications that range from aesthetic to highly functional - Decoration construction. hardware. Mechanical structure, chemical equipment, pulp and paper. aerospace, nuclear engineering and heat treating industries boiler, handrail, doors, windows, housewares,kitchenware,etc
stainless steel hexagonal tubing is included both welded and seamless
Featurues
good corrosion resistance, weld ability, machine ability, and can be easily cleaned and sterilized. It has excellent mechanical properties and presents the desirable combination of high strength and good work ability. Stainless tube is much lighter than its equivalent bar shape and therefore more practical for use in fabrication where weight is a concern.
Specifications -
| Standards | ASTM A554 |
| Dimensions | ASTM,AISI,ASME |
| Types | Rectangular |
| Material Grade | 301, 304, 304L,304LN,304N 305,309,309S,310,310S,316,316L.316LN, 316N,316Ti,317,317L,321,321H,347,347H, 904L |
Available sizes
| Size (axb) mm | Thickness mm |
| 13.8x15.9 | 1.0-1.8 |
| 16x18 | 1.0-1.8 |
| 17x19 | 1.0-1.8 |
| 19×22 | 1.0-1.8 |
| 22x25 | 1.0-1.8 |
| 31x32 | 1.0-1.8 |
| 33x38 | 1.0-1.8 |
| 49×50 | 1.0-1.8 |
| 5Sx62 | 1.0-1.8 |
| 5Sx63 | 1.0-1.8 |
| 67×76 | 1.0-1.8 |
Hot Tags: astm554 tp304 stainless steel square pipe welding, China astm554 tp304 stainless steel square pipe welding suppliers, Inconel 625 Alloy Steel Plate, SS410 Stainless Steel Pipe, 420J1 420J2 316 Stainless Pipe, 1 4509 1 4510 Pipes And Tubes, Stainless Steel High Pressure Pipe, 410 Stainless Steel Pipe