ASTM A789 DSS Tubing & ASTM A790 DSS Pipes
video

ASTM A789 DSS Tubing & ASTM A790 DSS Pipes

Duplex stainless steel tubing and pipes, either seamless or welded, are intended for services requiring general corrosion resistance, with particular emphasis on resistance to stress corrosion cracking. There are several prevalent duplex grades that can be readily sourced from most pipe mills: UNS S31803, UNS S32205, UNS S32750 and UNS S32760. Both S31803 and S32205 are designated as alloy 2205, while S32750 are designated as alloy 2507.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of astm a789 dss tubing & astm a790 dss pipes in China. If you're going to wholesale high quality astm a789 dss tubing & astm a790 dss pipes made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Duplex stainless steel tubing and pipes, either seamless or welded, are intended for services requiring general corrosion resistance, with particular emphasis on resistance to stress corrosion cracking. There are several prevalent duplex grades that can be readily sourced from most pipe mills: UNS S31803, UNS S32205, UNS S32750 and UNS S32760. Both S31803 and S32205 are designated as alloy 2205, while S32750 are designated as alloy 2507.

219 196

Duplex stainless steel tubing or tube, either seamless or welded, shall be manufactured in according with ASTM A789 (ASME SA-789), which is a hollow product of round or any other cross section having a continuous periphery. The tubing is produced to the actual outside diameter and minimum or average wall thickness specified by the purchaser. The wall thickness of tubing is normally given in decimal parts of an inch rather than as a fraction. When gauge numbers are given without reference to a system, Birmingham Wire Gauge (BWG) is implied.

 

Duplex stainless steel pipe, either seamless or straight-seam welded, shall be manufactured in accordance with ASTM A790 (ASME SA-790), which is a tube with a round cross section conforming to the dimensional requirements for nominal pipe size & schedule number as tabulated in ASME B36.10M and ASME B36.19M. For custom-designed special DSS pipe have diameter not listed in the above mentioned standards, the nominal diameter corresponds to the outside diameter and the actual wall thickness shall be specified.