ASTM A312 TP317 Stainless Steel ERW Pipe
Surface Condition:Ba, Annealing Pickling, Polished
Transport Package:Wooden Box
Stainless Steel Standar:ASTM A312
Wall Thickness:Sch 10s, 40s, 80s
Certificate:ISO 9001-2000,ASME,DNV
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of astm a312 tp317 stainless steel erw pipe in China. If you're going to wholesale high quality astm a312 tp317 stainless steel erw pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
ASTM TP317 stainless steel pipe is a grade of stainless steel produced according to the American ASTM standard. It is equivalent to my country's 0Cr19Ni13Mo3 stainless steel pipe. 317 contains 19% chromium, 13% nickel and 3% molybdenum.
ASTM TP317 stainless steel welded pipe is a high-alloyed austenitic stainless steel, whose chemical composition includes high chromium (Cr), nickel (Ni) and a small amount of molybdenum (Mo), niobium (Nb) and other elements.
TP317 stainless steel industrial pipe production process includes hot rolling, cold drawing, rolling, etc., and the delivery state can be heat treatment or pickling. Its specifications range from 6mm to 762mm in outer diameter, 1mm to 140mm in wall thickness, and 4m to 12m in length, and can be produced to a fixed length.
Products Data
Size: 3 inch.
Length: 6M.
Material: ASTM A312 TP317.
Wall Thickness: SCH 40.
Standard: ASTM A312.
End Type: Beveled End.
| Chemical Composition and Mechanical Property For ASTM A312 | ||||||||||||
| Steel Grade | Chemical Composition | Mechanical performance | ||||||||||
| C(Max) | Mn(Max) | P(Max) | S(Max) | Si(Max) | Cr | Ni | Mo | Tensile Strength (Min) |
Yield Strength (Min) |
|||
| psi | Mpa | psi | Mpa | |||||||||
| TP317 | 0.08 | 2.00 | 0.045 | 0.03 | 1.00 | 18.0–20.0 | 11.0–14.0 | 3.0–4.0 | 515 | 75 | 205 | 30 |
Products Display
ASTM A312 TP317 Round pipes

Why choosing GNEE
GNEE has an annual production line of 25,000 tons of stainless steel seamless pipes, 20,000 tons of welded pipes, and 5,000 tons of pipe fittings. It can produce φ6~φ762×0.5~70mm stainless steel seamless pipes, φ15~φ2200×0.5~80mm stainless steel welded pipes, pipe fittings and other products according to GB, ASTM, JIS, DIN and other standards.
please contact us for a quote! ss@gneesteel.com
PRODUCTS TESTING

GNEE FACTORY ENVIRONMENT

GNEE PACKAGING AND SHIPPING

FAQ
Q.Do you have MOQ?
A.Depends on different ideas, Can be negotiated.The larger the quantity is, the competitive the unit price will be.
Q.Do you have quality control?
A.Yes, we have got BV.SGS certification.
Q.Where are you located? Can I visit you?
A.Sure, you are welcome to visit our factory anytime.
Hot Tags: astm a312 tp317 stainless steel erw pipe, China astm a312 tp317 stainless steel erw pipe suppliers, SS410 Stainless Steel Pipe, Slip On Flanges, 1 4509 1 4510 Pipes And Tubes, Inconel 625 Alloy Steel Plate, 410 Stainless Steel Pipe, Stainless Steel High Pressure Pipe
You Might Also Like
Send Inquiry