ASTM A312 TP316 Stainless Steel Round Pipe
Surface Condition:Ba, Annealing Pickling, Polished
Transport Package:Wooden Box
Specification:6 - 114.3 mm
Certificate:ISO 9001-2000,ASME,DNV
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of astm a312 tp316 stainless steel round pipe in China. If you're going to wholesale high quality astm a312 tp316 stainless steel round pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
ASTM A312 TP316 stainless steel round pipe is an austenitic stainless steel pipe specified by the ASTM A312 standard, mainly used for seamless and welded austenitic stainless steel.
GNEE supplies ASTM A312 TP316 stainless steel pipes including TP316 stainless seamless pipes and TP316 stainless welded pipes with excellent corrosion resistance, high temperature strength and good processing performance. And before leaving the factory, X-ray flaw detection, ultrasonic testing and other technologies are used to ensure that there are no defects inside the pipe.
Products Data
Chemical Composition Of ASTM A312 TP 316 Stainless Steel ERW Pipe
| GRADE |
C |
MN |
SI |
P |
S |
CR |
MO |
NI |
N |
|
|---|---|---|---|---|---|---|---|---|---|---|
|
316 |
Min |
- |
- |
- |
0 |
- |
16.0 |
2.00 |
10.0 |
- |
|
Max |
0.08 |
2.0 |
0.75 |
0.045 |
0.03 |
18.0 |
3.00 |
14.0 |
0.10 |
Mechanical Properties Of ASTM A312 TP 316 Stainless Steel Seamless Pipe
| GRADE | TENSILE STR (MPA) MIN |
YIELD STR 0.2% PROOF (MPA) MIN |
ELONG (% IN 50MM) MIN |
HARDNESS | |
|---|---|---|---|---|---|
| ROCKWELL B (HR B) MAX | BRINELL (HB) MAX | ||||
|
316 |
515 |
205 |
40 |
95 |
217 |
Products Display
ASTM A312 TP316 Cold Drawn Steel Pipe

Why choosing GNEE
GNEE has 25 sets of various mechanical equipment for precision manufacturing of steel pipes, including 15 cold rolling mills, 10 cold drawing mills, and two sets of heat treatment furnaces.
The stainless steel pipes produced by GNEE have made our company a qualified supplier for many companies for several consecutive years. In addition to being sold domestically and abroad, our products are also exported to South Korea, India, Indonesia, Pakistan, Vietnam, Brazil, Thailand and many other overseas markets.
If you have any inquiry, please don't hesitate to contact us immediately! Free Quote ss@gneesteel.com
GNEE CUSTOMER VISIT

GNEE FACTORY ENVIRONMENT

GNEE PACKAGING AND SHIPPING

FAQ
1.Q: Do you provide customized product services?
A: Of course, we can design and produce the products you need based on your specifications and drawings. For example: special dimensions, special controls, OEM, etc.
2.Q: Are you a manufacturer or trader?
A: We are manufacturers. We have our own factory to produce and process various kinds of stainless steel /nickel alloy pipes.
Hot Tags: astm a312 tp316 stainless steel round pipe, China astm a312 tp316 stainless steel round pipe suppliers, Slip On Flanges, Stainless Steel High Pressure Pipe, SS410 Stainless Steel Pipe, 420J1 420J2 316 Stainless Pipe, Inconel 625 Alloy Steel Plate, 1 4509 1 4510 Pipes And Tubes
You Might Also Like
Send Inquiry