Annealed Pickled Stainless Steel Seamless Pipe ASTM A269 12*1.5 Bright BA Surface
video

Annealed Pickled Stainless Steel Seamless Pipe ASTM A269 12*1.5 Bright BA Surface

BA Surface Stainless Steel Seamless Pipe SUS316L ASTM A312 TP316L 12*1.5 Description Application: Construction,Decoration,Industry,boiler,Chemical Standard: DIN,ASTM,JIS,AISI Steel Grade: 304 304L 316 316L 310S 321 Type: Seamless Welding Line Type: Seamless Thickness: 1mm-20mm Length: 3000mm~6000mm Shape: Round Pipe Tube Outer Diameter: 6-762mm Technique: Cold Drawn Material: Stainless Steel,300 Series Finish: Polished,Ba,pickled High Light: BA Surface Stainless Steel Seamless Pipe , SUS316L Stainless Steel Seamless Pipe , 12*1.5 Stainless Steel Seamless Pipe
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of annealed pickled stainless steel seamless pipe astm a269 12*1.5 bright ba surface in China. If you're going to wholesale high quality annealed pickled stainless steel seamless pipe astm a269 12*1.5 bright ba surface made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Annealed Pickled Stainless Steel Seamless Pipe ASTM A269 12*1.5 Bright BA Surface

Description

Application: Construction,Decoration,Industry,boiler Standard: DIN,ASTM,JIS,AISI
Steel Grade: 304 304L 316 316L 310S 321 Type: Seamless
Welding Line Type: Seamless Thickness: 1mm-20mm
Length: 3000mm~6000mm,Customer Request Shape: Round.square.Rectangle
Outer Diameter: 6-762mm Technique: Cold Drawn
Surface: Annealing,pickling,polishing Material: 200 Series/300 Series/400series
Grade: 304L 316 316L 310s 321 321H 347 347H Finish: Polished,Ba,pickled
High Light:

Annealed Pickled Stainless Steel Seamless Pipe

,

ASTM A269 Stainless Steel Seamless Pipe

,

12*1.5 Stainless Steel Seamless Pipe

SUS304 TP304 12*1.5 Stainless Steel Seamless Pipe Bright Annealed BA Surface

 

Our quality policy is to continuously improve the quality management system, provide high-performance seamless 1/4 Stainless Steel Instrument Tube, cold drawn Electro Polished Pipes, seamless Natural Gas Annealed Stainless Steel Pipes and constantly meet customers' demands and expectations for product quality. We embody our corporate social responsibility in a series of actions to improve our own connotation and actively return to society. Communication and execution, team innovation, satisfaction and win-win are our business philosophy and purpose.

 

 

Seamless stainless steel bright annealed tube is a kind of heat treatment and surface delivery requirements in the production process of steel pipes. The heat treatment is in the state of protective gas (H2+N2 mixed gas), and the temperature control range is 1010-1100 degrees Celsius. It is seamless for clean cleaning. The stainless steel tube is annealed. This heat-treated stainless steel pipe has excellent surface quality, good mechanical properties, and strong bending plasticity, which is convenient for customers to perform various bending, welding, Lok connection and other processing.

 

Bright annealing heat treatment can be applied to the manufacturing process of instrument pipes, hydraulic pipes, high-pressure pipes, precision pipes, fluid conveying pipes, high-purity gas/bulk gas conveying pipes, automobile pipes and other industries. The inner surface of bright annealed steel pipes is clean and free. Oil, no impurities, no falling particles, corrosion resistance and other properties can meet the pollution-free transportation of various fluid media.

 

Details of the bright annealing tube manufactured by KC-SCT

Strict production control system:

-Cold rolled or cold drawn control tolerance

-Excellent oil control and grease removal technology

-Strictly monitor the natural gas heat treatment process and bright heat treatment.

-Environmental protection and efficient pickling passivation + neutralization + cleaning

-A rigorous quality inspection team (dimension inspection, surface inspection, non-destructive inspection, mechanical performance inspection, metallographic inspection)

 

1. Material

Standard Grade
UNS S31603 S31600 S31635 S30400 S30403 S32100
ASTM/ANSI TP316L TP316 TP316ti TP304 TP304L TP321
ISO/EN 1.4404 1.4401 1.4571 1.4301 1.4306 1.4541
JIS SUS316L SUS316 SUS SUS304 SUS304L SUS321
GB S31603 S31608 S31668 S30408 S30403 S32168

 

The materials listed above are often manufactured, and materials within national standards can also be provided for manufacturing.

 

2. Standard

Standard
ASTM/ANSI A269 A270 A312 A213 A789 A632 A790  
ISO/EN/DIN EN 10305-1 EN 1127 DIN 11850 DIN 2470 DIN 10216-5 DIN 10208 DIN 10297-2 ISO 2037
JIS G3447 G3459 G3463 G3464 G7222      
GB 14976 13296 18984 3090 3093 3639    

 

3. Specification

Standard Diameter Wall thinkness
in mm in mm
ASTM A269A270A632A213 1/8"~2" 3.18~50.8 0.15"~0.12" 0.4~3.05
A312 1/8"~2" 10.3~60.3 5S,10S,40S
ISO/EN/DIN 1127 / 3.0~60.3 / 0.4~4.0
JIS G3447 1/2"~2" 12.7~50.8   1.2~2.0
G3459 1/8~2(6A~50A) 10.5~60.5 5S,10S,40S
G3463G3464 / 15.9~60.3 / 1.2~4.0
GB 14976 / 3.0~60.3 / 0.4~4.0

 

#It is possible to customize pipes with outside diameter and wall thickness not specified in the standard;

 

4. Tolerance

The tolerances of the outer diameter and wall thickness of the pipes produced in accordance with the standards can also be agreed with the purchaser separately;

Special (non-standard) pipe tolerances for outer diameter and wall thickness can be more precise.

 

5. Surface delivery status

Bright annealing: atmosphere protection heat treatment, the inner and outer surfaces are bright and smooth.

Bright annealed tube customization can make requirements for the roughness or polishing of the inner and outer surfaces:

 

 

Inside surface Outside surface
Roughness (BA) Polishing mesh
(MPBA)
Roughness Polishing mesh
≤Ra0.4um ≤Ra0.8um 240#
320#
400#
≤Ra0.4um ≤Ra0.8um 240#
320#
400#

 

 

The accuracy of the inner and outer surface roughness of bright annealed steel pipes can be met by mechanical polishing or without mechanical polishing;

 

6. Clean cleaning process

The steel pipe manufacturing process adopts ultrasonic + degreasing cleaning process to effectively remove various pollutants generated in the pipeline manufacturing.

 

7. Non-destructive inspection

Each stainless steel pipeline is tested according to the standard of water pressure testing and eddy current testing:

Hydrostatic pressure detection: maximum pressure 20Mpa, time 5 seconds

Eddy current flaw detection: Perform inspection according to standard sample tubes, and comply with standards such as ASTM, JIS, ISOENDIN, GB, etc.

 

8. Other inspections

Perform random inspections of stretching, flattening, flaring, grain size, hardness, etc. according to the standard.

With advanced technology, relentless pursuit for innovation and dedicated engineers, we have become the professional TP304/304L 8mmx1mm Bright Annealing Seamless Stainless Steel Tube for Instrument, Chromatography, Hydraulic manufacturer with a full range of products line. 'Developing customers with integrity, supplying high quality products with the most competitive price and the shortest delivery time, serving them with heart and soul' is the philosophy of our company. Welcome your enquiry! We continue to absorb and introduce various professional technical and management talents, hoping to enrich the management team and strengthen technical productivity, so that our company can achieve long-term development.

 

Hot Tags: bright annealed tubing, China, suppliers, manufacturers, factory, wholesale, price, cost, size, seamless, cold drawn, made in China, seamless Annealed Pickled Stainless Steel Pipes, cold drawn 316L Medical Tubes, seamless Pressure Stainless Steel Precision Tubes, seamless Hydraulic Tube, Oil And Gas Stainless Steel Hydraulic Tube SIZE, cold drawn Stainless Steel Tubes

Annealed Pickled Stainless Steel Seamless Pipe ASTM A269 12*1.5 Bright BA Surface 0Annealed Pickled Stainless Steel Seamless Pipe ASTM A269 12*1.5 Bright BA Surface 1Annealed Pickled Stainless Steel Seamless Pipe ASTM A269 12*1.5 Bright BA Surface 2

Hot Tags: annealed pickled stainless steel seamless pipe astm a269 12*1.5 bright ba surface, China annealed pickled stainless steel seamless pipe astm a269 12*1.5 bright ba surface suppliers, 420J1 420J2 316 Stainless Pipe, 1 4509 1 4510 Pipes And Tubes, 410 Stainless Steel Pipe, SS410 Stainless Steel Pipe, Slip On Flanges, Stainless Steel High Pressure Pipe

Send Inquiry

whatsapp

Phone

E-mail

Inquiry