440B 431 410J1 Stainless Steel Square Tube
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 440b 431 410j1 stainless steel square tube in China. If you're going to wholesale high quality 440b 431 410j1 stainless steel square tube made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
440B 431 410J1 Stainless Steel Square Tube
440B 431 410J1 ss seamless tube
You can get a better understanding of the Customizable 440B 431 410J1 ss square tube here.
440B ss steel is a high carbon martensitic stainless steel with good strength, moderate corrosion resistance and the ability to obtain and maintain wear resistance and excellent corrosion resistance.
431 ss pipe seamless is a high-chromium, low-nickel, high-hardenability martensitic stainless steel with high strength and good corrosion resistance, usually hardened in the tensile range 850-1000 MPa (condition T) Brinell range 248-302 and Tempering.
410 stainless pipe is a stainless steel grade produced in accordance with American ASTM standards. It is equivalent to my country's 1Cr13 stainless steel, S41000 (American AISI, ASTM), containing 0.15% carbon and 13% chromium. 410 smls pipe: has good corrosion resistance and mechanical processing properties, general purpose blades, valves.
440B 431 410J1 ss square tube Description
|
Mechanical Properties |
||||||
|
Grade (UNS) |
Tensile Strength (MPa) ≥ |
Yield Strength, 0.2%, ≥ (MPa) |
Elongation in 50 mm (%) ≥ |
Reduction in area (%) |
Hardness |
Product & Condition |
|
440A (S44002) |
725 |
415 |
20 |
95 HRB |
Annealed bar |
|
| 1790 |
1650 |
5 |
20 |
51 HRC |
Bars tempered at 315 °C |
|
|
≤ 965 |
Annealed wire, cold finished |
|||||
|
440B (S44003) |
740 |
425 |
18 |
96 HRB |
Annealed bar |
|
|
1930 |
1860 |
3 |
15 |
55 HRC |
Bars tempered at 315 °C |
|
|
≤ 965 |
Annealed wire, cold finished |
|||||
|
440C (S44004) |
760 |
450 |
14 |
97 HRB |
Annealed bar |
|
|
1970 |
1900 |
2 |
10 |
57 HRC |
Bars tempered at 315 °C |
|
|
≤ 965 |
Annealed wire, cold finished |
|||||