Stainless Steel Schedule 40 1.4439 Pipe Reducer
video

Stainless Steel Schedule 40 1.4439 Pipe Reducer

Schedule 40 butt weld fittings connect with medium-pressure (300-999 psi) pipe. Butt weld (BW) fittings form pipe joints with strength, fatigue, corrosion resistance, and temperature compliance. These beveled fittings are welded to the ends of same thickness Schedule 40 stainless steel unthreaded pipe.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of stainless steel schedule 40 1.4439 pipe reducer in China. If you're going to wholesale high quality stainless steel schedule 40 1.4439 pipe reducer made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Schedule 40 ss  fittings are Nominal Pipe Size (NPS), not Tube Outside Diameter (OD). The walls of Schedule 40 pipe and fittings are almost twice as thick as standard 16 gauge Tube OD fittings, making them ideal for custom turbo manifolds and downpipe fabrication. The increased wall thickness provides added durability and is less prone to cracking under the high thermal stress from exhaust gas temperatures.Additional buttweld pipe fittings are available in long radius 45's, short and long radius 90's, tee's and straight lengths for making anything from log style manifolds to equal length twin scroll manifolds. Great for use in conjunction with Vibrant Turbo Manifold Merge Collectors and 1/2" Thick Mild Steel Manifold Flanges which are optimized for Sch. 40 fittings.

reducerstainless reducer

1.4439  Schedule 40 fittings Chemical Composition 

Weight % C Mn P S Si Cr Ni Mo N Cu
Min.           19,0 24,0 3,00   1,20
Max. 0,020 1,20 0,030 0,010 0,70 21,0 26,0 4,50 0,50 2,00

 

1.4439 Schedule 40 ss reducer  fittings Mechanical Properties (Typical)

  Yield strength Rp0.2,
MPa
Yield strength Rp1.0,
MPa
Tensile strength Rm,
MPa
Elongation
[%]
Hardness
[HB]
ASTM A240 ≥ 230   520 – 720 ≥ 35 ≤ 90
PLATE CR (COIL) ≥ 240 ≥ 270 530 – 730 ≥ 35 ≤ 90
PLATE HR (COIL) ≥ 220 ≥ 260 530 – 730 ≥ 35 ≤ 90
PLATE (QUARTO) ≥ 220 ≥ 260 520 – 720 ≥ 35 ≤ 90

 

Customer Visit 

GNEE Steel is a professional stainless steel supplier, providing high-quality stainless steel pipes, stainless steel coils, stainless steel plates, stainless steel pipe fittings, and other stainless steel products.Over the last 30 years, we have been serving our clients, we have built a strong clientele across 32 countries and 15 industrial verticals, right from basic industries such a paper to highly demanding offshore services.

gnee steelgnee steel

 

Hot Tags: stainless steel schedule 40 1.4439 pipe reducer, China stainless steel schedule 40 1.4439 pipe reducer suppliers, 310 Butt Weld Flanges, Super Duplex Steel UNS S32750 Angle