SS446 Alloy Stainless Steel Fittings
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of ss446 alloy stainless steel fittings in China. If you're going to wholesale high quality ss446 alloy stainless steel fittings made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
SS446 Alloy Stainless Steel Fittings

This alloy is commonly used between temperatures ranging from 1500 Deg F to 2100 Deg F, although the elevated temperature strength is lower. 446 SS alloy is the heat resistant alloy that tolerates molten brass and copper. As with the high chromium ferritic stainless, this grade embrittles severely in the temperature ranging 700 deg F to 1000 deg F. Alloy SS 446 should be used at this temperature unless full room temperature ductility loss might be tolerated. Sigma phase embrittlement might occur upon long exposure in the temperature ranging from 100 Deg F to 1300 Deg F. Stainless steel 446 alloy is highly malleable to the brittle impact transition temperature.
Hot Tags: ss446 alloy stainless steel fittings, China ss446 alloy stainless steel fittings suppliers, Super Duplex Steel UNS S32750 Angle, 310 Butt Weld Flanges
Previous
S32550 Stainless Steel AngleYou Might Also Like